首页> 外国专利> ANISOTROPIC POLYIMIDE ORIENTED FILM IN WHICH IN-PLANE ORIENTATION IS DERIVED BY LIGHT IRRADIATION, A MANUFACTURING METHOD THEREOF, AND A BOARD FOR FLEXIBLE DISPLAY USING THE SAME

ANISOTROPIC POLYIMIDE ORIENTED FILM IN WHICH IN-PLANE ORIENTATION IS DERIVED BY LIGHT IRRADIATION, A MANUFACTURING METHOD THEREOF, AND A BOARD FOR FLEXIBLE DISPLAY USING THE SAME

机译:平面取向的各向异性聚酰亚胺薄膜是通过光辐照,其制造方法以及使用该面板进行柔性显示的面板来推导的

摘要

PURPOSE: An anisotropic polyimide oriented film is provided to impart low thermal expansion coefficient of 20 ppm/°C or lower by controlling orientation in surface of a polyimide film, thereby suitable for a flexible display substrate.;CONSTITUTION: An anisotropic polyimide oriented irradiates with light a polyimide film containing a polymer liquid crystal material, which has polyimide as a backbone, a photo-crosslinkable group in side chain so that orientation in surface is increased. A manufacturing method of synthesizing polyamic acid solution comprises a step of synthesizing polyamic acid solution through condensation polymerizing aromatic tetracarboxylic dianhydride, and aromatic diamine; a step of obtaining a blending solution by adding a polymer with 10-20 weight% of photo-crosslinkable group into the polyamic acid solution; a step of manufacturing a film by imidizing the blending solution; and a step of irradiating the film with light, and heat-treating the same.;COPYRIGHT KIPO 2012
机译:目的:提供一种各向异性的聚酰亚胺取向膜,通过控制聚酰亚胺膜表面的取向使其具有20 ppm /℃或更低的低热膨胀系数,从而适用于柔性显示基板。;组成:各向异性的聚酰亚胺取向的辐射体光照下,含有以聚酰亚胺为骨架的聚合物液晶材料的聚酰亚胺膜,侧链中的光可交联基团增加了表面取向。合成聚酰胺酸溶液的制造方法包括以下步骤:通过使芳族四羧酸二酐和芳族二胺缩聚来合成聚酰胺酸溶液。通过向聚酰胺酸溶液中添加具有10〜20重量%的光交联性基团的聚合物而得到混合溶液的步骤。通过使混合溶液酰亚胺化来制造膜的步骤;以及用光照射胶片并对其进行热处理的步骤。; COPYRIGHT KIPO 2012

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号