MANUFACTURING METHOD OF POLYOLEFINS WITH EXCELLENT FULL NOTCH CREEP TEST AND IMPROVED SAGGING TIME BY USING A MOLECULAR WEIGHT CONTROLLING AGENT, AND A POLYOLEFIN THEREOF

机译:分子重量控制剂,具有出色的全缺口蠕变试验和改善的下陷时间的聚烯烃制造方法及其聚烯烃

摘要

PURPOSE: A manufacturing method of polyolefin is provided to able to provide polyolefin which is especially suitable for blow molding because of low polymer melt index(MI), high polydispersity(PDI) and high full notch creep test to density or polymer melt index.;CONSTITUTION: A manufacturing method of polyolefin comprises a step of polymerizing olefin under the presence of a metallocene catalyst and a molecular weight controller. The polymerization is conducted in a cascade-CSTR reactor. The cascade-CSTR reactor comprises a first reactor, a second reactor and a post reactor. Polyolefin is manufactured by the manufacturing method, has multi-modal molecular weight distribution, and has weight average molecular weight of 100,000-700,000.;COPYRIGHT KIPO 2013;[Reference numerals] (AA) First reactor; (BB) Second reactor; (CC) Post reactor
机译:目的:提供一种聚烯烃的制造方法,以提供一种特别适用于吹塑的聚烯烃,因为它具有低的聚合物熔体指数(MI),高的多分散性(PDI)和高的密度或聚合物熔体指数的全缺口蠕变试验。组成:聚烯烃的制造方法包括在茂金属催化剂和分子量控制剂存在下聚合烯烃的步骤。聚合在级联CSTR反应器中进行。级联-CSTR反应器包括第一反应器,第二反应器和后反应器。聚烯烃通过制造方法制造,具有多峰分子量分布,重均分子量为100,000-700,000。; COPYRIGHT KIPO 2013; [参考数字](AA)第一反应器; (BB)第二反应堆; (CC)后反应堆

著录项

  • 公开/公告号KR20120111530A

    专利类型

  • 公开/公告日2012-10-10

    原文格式PDF

  • 申请/专利权人 LG CHEM. LTD.;

    申请/专利号KR20110030050

  • 申请日2011-04-01

  • 分类号C08F10/00;C08F2/01;C08F4/6592;B29C49/00;

  • 国家 KR

  • 入库时间 2022-08-21 17:09:03

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号