PURPOSE: A cement reducing agent and high strength curing method using the same are provided to minimize use amount of cement and prevent strength degradation. CONSTITUTION: A cement reducing agent comprises 10-15 parts by weight of KCL, 5-10 parts by weight of sodium chloride, 5-10 parts by weight of ammonium chloride, 1-5 parts by weight of nickel chloride, 1-5 parts by weight of cobalt chloride, 20-30 parts by weight of sodium carbonate, and 5-15 parts by weight of potassium carbonate. A high strength curing method of construction comprises the following steps: manufacturing cement reducing agent(s10); manufacturing a mixture by mixing 100 parts by weight of aggregate and 1-10 parts by weight of the cement reducing agent(s20); dry-mixing after putting 16-25 parts by weight of water into the mixture(s30); and installing and curing the mixture(s40). [Reference numerals] (S10) Manufacturing cement reducing agent; (S20) Manufacturing a mixture (aggregate, cement, cement reducing agent); (S30) Mixing and agitating after adding water; (S40) Installing and during the mixture
机译:目的:提供一种水泥还原剂和使用该水泥还原剂的高强度固化方法,以最大程度地减少水泥的用量并防止强度降低。组成:水泥还原剂包括10-15重量份的KCL,5-10重量份的氯化钠,5-10重量份的氯化铵,1-5重量份的氯化镍,1-5份重量的氯化钴,20-30重量份的碳酸钠和5-15重量份的碳酸钾。一种高强度固化方法,包括以下步骤:制造水泥还原剂(s10);通过混合100重量份的骨料和1-10重量份的水泥还原剂来制造混合物;将16-25重量份的水倒入混合物中后进行干混(s30);并安装并固化混合物。 [附图标记](S10)制造水泥还原剂; (S20)制造混合物(骨料,水泥,水泥还原剂); (S30)加水搅拌混合; (S40)安装和混合期间

著录项

  • 公开/公告号KR20120113015A

    专利类型

  • 公开/公告日2012-10-12

    原文格式PDF

  • 申请/专利权人 KIM BYUNG MAN;

    申请/专利号KR20110030674

  • 发明设计人 KIM BYUNG MAN;

    申请日2011-04-04

  • 分类号C04B22/12;C04B22/10;C04B40;C04B40/02;

  • 国家 KR

  • 入库时间 2022-08-21 17:08:57

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号