首页> 外国专利> COMPOSITION CAPABLE OF FORMING YELLOWING-FREE, LOW-HARDNESS POLYURETHANE ELASTOMER, AND METHOD FOR PRODUCING YELLOWING-FREE, LOW-HARDNESS POLYURETHANE ELASTOMER USING THE SAME

COMPOSITION CAPABLE OF FORMING YELLOWING-FREE, LOW-HARDNESS POLYURETHANE ELASTOMER, AND METHOD FOR PRODUCING YELLOWING-FREE, LOW-HARDNESS POLYURETHANE ELASTOMER USING THE SAME

机译:能够形成无黄,低硬度的聚氨酯弹性体的组成以及使用该方法制备无黄,低硬度的聚氨酯弹性体的方法

摘要

The present invention provides a non-yellowing, low hardness without the use of plasticizers Donna non-bleeding properties (bleeding-free property) is achieved, tack (tack) is small, and that the hardness variation as a function of temperature provides a thermosetting polyurethane elastomer in a small problem. If the present invention is to include a plasticizer standing, and also characterized in that said (A) isocyanate-terminated prepolymer and (B) a polyester polyol shown below. (A) isocyanate-terminated prepolymer: hexane diisocyanate with a molecular weight of 500 or less branched alkyl group-containing glycol obtained via a process of reacting an isocyanate-terminated prepolymer. (B) polyol polyester: trimethylolpropane, obtained from 3-methyl-1,5-pentanediol and adipic acid, average functional group number = 2.5 to 3.5, a polyester polyol having a number average molecular weight of from 800 to 5000
机译:本发明在不使用增塑剂的情况下提供了不黄变的,低硬度的唐娜(Donna)具有非渗色性(无渗色性),粘性(粘性)小,并且随温度变化的硬度变化提供了热固性聚氨酯弹性体的一个小问题。如果本发明包括增塑剂,并且其特征还在于,所述(A)异氰酸酯封端的预聚物和(B)如下所示的聚酯多元醇。 (A)异氰酸酯封端的预聚物:通过使异氰酸酯封端的预聚物反应的方法获得的,分子量为500以下的含支链烷基的二醇的己二酸二异氰酸酯。 (B)多元醇聚酯:由3-甲基-1,5-戊二醇和己二酸制得的三羟甲基丙烷,平均官能团数= 2.5至3.5,数均分子量为800至5000的聚酯多元醇

著录项

  • 公开/公告号KR101118979B1

    专利类型

  • 公开/公告日2012-03-13

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20097019007

  • 申请日2008-03-14

  • 分类号C08G18/42;C08G18/10;C08G18/71;

  • 国家 KR

  • 入库时间 2022-08-21 17:08:32