首页> 外国专利> NI-BASED ALLOY WELDED STRUCTURE AND HEAT EXCHANGER HAVING HIGH-TEMPERATURE CORROSION RESISTANCE

NI-BASED ALLOY WELDED STRUCTURE AND HEAT EXCHANGER HAVING HIGH-TEMPERATURE CORROSION RESISTANCE

机译:具有高温耐腐蚀性能的基于镍的合金焊接结构和换热器

摘要

Corrosion and Si- exhibits high corrosion resistance in an environment of high-temperature corrosion between the Ni-based alloy weld and increase the high-temperature corrosion resistance in the vicinity, and provides high temperature corrosion welding Ni-based alloy structure within the available long-term under high temperature corrosive environments. ; Ni: 45 to 57wt%, Cr: 23 to 35wt%, Mo: 1 to 5wt%, Si: 3 to 6wt%, C: contains 0.05 to 0.5wt%, and the balance of Fe and Ni-based alloy as the high temperature corrosion within the welding structure between the plurality of elements within the high temperature corrosion member formed by a Ni-based alloy consisting of unavoidable impurities and Si- weld joint is formed, wherein the welding welds the welding metal, and some of the Si - the first high-temperature corrosion Ni-based alloy weld metal toughness is higher than (WM1), and the rest is in the high-temperature corrosion Si- second deposition of Ni-based alloys with the same composition, metal (WM2), exposure to high temperature corrosive atmosphere the second metal being deposited on the surface (WM2) is characterized in that the exposed.
机译:腐蚀和Si-在Ni基合金焊缝之间的高温腐蚀环境中表现出高耐腐蚀性,并增加附近的高温腐蚀抗性,并在可用的长时间内提供高温腐蚀焊接Ni基合金结构高温腐蚀环境下长期使用。 ; Ni:45〜57wt%,Cr:23〜35wt%,Mo:1〜5wt%,Si:3〜6wt%,C:含有0.05〜0.5wt%,Fe和Ni基合金的余量高。在由由不可避免的杂质组成的Ni基合金和Si-焊接接头形成的高温腐蚀构件内的多个元件之间的焊接结构内的高温腐蚀形成,其中,焊接将焊接金属和一些Si-焊接在一起。第一次高温腐蚀镍基合金焊缝的金属韧性高于(WM1),其余的是在高温腐蚀Si中第二次沉积具有相同成分,金属(WM2)的镍基合金在高温腐蚀气氛下,沉积在表面(WM2)上的第二种金属的特征在于暴露在外。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号