FIELD: metallurgy.;SUBSTANCE: complex alloy containing alloying elements, wt %, is melted by the aluminothermic method: molybdenum 25-27, vanadium 25-27, chromium 14-16, titanium 9-11, aluminium - balance, preparation of a charge containing the complex alloy, iron and zirconium in the form of technically pure metals, melting of an ingot of pseudo β-titanium alloy, at least by double remelting, at the same time the first remelting is carried out in a vacuum arc furnace or by the wall accretion method - a consumable electrode, and the second remelt - in the vacuum arc furnace.;EFFECT: invention makes it possible to produce a pseudo β-titanium alloy, which is highly homogeneous in its chemical composition and alloyed with refractory elements, with low aluminium content, having stable high-strength properties in combination with high impact strength.;2 ex
机译:领域:冶金;物质:通过铝热法熔化含有合金元素(重量百分比)的复杂合金:钼25-27,钒25-27,铬14-16,钛9-11,铝-天平,制备铝包含复杂合金,技术上纯净金属形式的铁和锆,至少通过两次重熔熔融拟β-钛合金锭的装料,同时第一次重熔在真空电弧炉或通过壁积方法-消耗电极和第二熔体-在真空电弧炉中进行。效果:本发明可以生产伪β-钛合金,该伪钛合金的化学成分非常均匀,并与耐火元素合金化;铝含量低,具有稳定的高强度性能和高冲击强度。; 2 ex

著录项

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号