FIELD: metallurgy.;SUBSTANCE: prior to high-temperature heating the isothermal annealing is performed at temperature of 1000°C with exposure during 0.5-1.0 hour, and high-temperature and cooling is performed cyclically; at that, in each cycle the heating is performed to the temperature which is lower by 40-50°C than solidus temperature; cooling is performed, except for the last cycle, to the temperature of 1000°C, and in the last cycle the cooling is performed to the temperature of 200°C; then in the air - to the room temperature.;EFFECT: invention allows increasing the degree of decarbonisation, degassing, cleaning from sulphur, colour impurities, non-metallic inclusions and reducing chrome evaporation at reducing the processing duration.;3 tbl
机译:领域:冶金;物质:在高温加热之前,在1000-C的温度下进行等温退火,并在0.5-1.0小时内进行暴露,并且高温和冷却循环进行。此时,在每个循环中进行加热至比固相线温度低40-50℃的温度。除了最后一个循环,进行冷却至1000℃的温度,并且在最后一个循环中,进行冷却至200℃的温度。效果:发明可以提高脱碳,脱气,清除硫,颜色杂质,非金属夹杂物的程度,并在减少处理时间的同时减少铬的蒸发。3tbl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号