首页> 外国专利> METHOD OF PRODUCING POLYESTERPOLYOLS WITH FUNCTIONALITY FROM 1,95 TO 3,25 AND HYDROXYL NUMBER FROM 90 TO 33 mg KOH/g AND USE THEREOF

METHOD OF PRODUCING POLYESTERPOLYOLS WITH FUNCTIONALITY FROM 1,95 TO 3,25 AND HYDROXYL NUMBER FROM 90 TO 33 mg KOH/g AND USE THEREOF

机译:制备功能度为1.95至3.25,羟值为90至33 mg KOH / g的聚酯多元醇的方法及其用途

摘要

FIELD: chemistry.;SUBSTANCE: present invention relates to method of producing polyesterpolyols with functionality from 1.95 to 3.25 and hydroxyl number from 90 to 33 mg KOH/g. The method is realised in two steps. The first step involves reaction of organic polycarboxylic acids with organic polyols at temperature 150-250°C to obtain a polyesterpolyol with hydroxyl number from 100 to 40 mg KOH/g and functionality from 1.95 to 3.25. At the second step, cyclic ester monomers are added to the obtained polyesterpolyol at temperature lower than 220°C and weight ratio from 10:1 to 1:1. After at most 60 minutes, the temperature must be lower than or equal to 175°C. The hydroxyl number of polyesterpolyol drops by at least 5 mg KOH/g. The molar ratio of the cyclic ester monomer to hydroxyl groups of the polyesterpolyol ranges from 0.75:1 to 10:1.;EFFECT: obtaining low-viscosity polyesterpolyols using a simple and cheap method.;4 tbl, 6 ex
机译:聚酯多元醇的制备方法技术领域本发明涉及官能度为1.95-3.25且羟值为90-33mg KOH / g的聚酯多元醇的制备方法。该方法分两个步骤实现。第一步涉及有机多元羧酸与有机多元醇在150-250°C的温度下反应,以获得羟基值为100至40 mg KOH / g,官能度为1.95至3.25的聚酯多元醇。在第二步骤中,将环状酯单体在低于220℃的温度和10:1至1:1的重量比下添加至获得的聚酯多元醇。最多60分钟后,温度必须低于或等于175°C。聚酯多元醇的羟值下降至少5mg KOH / g。环状酯单体与聚酯多元醇的羟基的摩尔比为0.75:1至10:1。效果:使用一种简单而廉价的方法获得低粘度聚酯多元醇。4tbl,6 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号