PROBLEM TO BE SOLVED: To provide a whisker crystal of iron-based superconductor which exhibits superconductivity at an absolute temperature of about 30 K, and to provide a production method which is easy to cope with toxicity and can industrially advantageously produce the whisker crystal.;SOLUTION: A mixed powder comprising raw materials constituted of a metal arsenide powder and a metal powder and an additive for promoting crystal growth is filled in a capsule-shaped reaction vessel made of metal. Then, a pressure of 240-380 MPa is mechanically applied via two punches arranged oppositely to each other. After depressurizing, the temperature of the reaction vessel is kept within the range of 700-1,000°C for ≥48 h. Successively, the reaction vessel is furnace cooled to 700°C or less at a fixed temperature lowering rate of ≤0.3°C/min.;COPYRIGHT: (C)2013,JPO&INPIT
机译:解决的问题:提供铁基超导体的晶须晶体,其在约30K的绝对温度下显示出超导性,并提供一种易于应对毒性并且可以在工业上有利地生产该晶须晶体的生产方法。解决方案:将由金属砷化物粉末和金属粉末组成的原材料与用于促进晶体生长的添加剂混合而成的粉末填充到由金属制成的胶囊状反应容器中。然后,通过彼此相对布置的两个冲头机械地施加240-380MPa的压力。减压后,将反应容器的温度在700-1,000°C的范围内保持≥48小时。随后,以≤0.3°C / min的固定降温速率将反应容器炉冷至700°C或以下;版权所有:(C)2013,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号