PROBLEM TO BE SOLVED: To provide steel for high strength welded structure which has excellent toughness in an ultrahigh heat input weld part HAZ (heat affected zone), and to provide its production method.;SOLUTION: The high strength steel for welded structure having the excellent toughness in the ultrahigh heat input weld part HAZ has a composition comprising, by mass%, 0.01 to 0.20% C, 0.02 to 0.50% Si, 1.5 to 3.5% Mn, ≤0.03% P, 0.005 to 0.030% S, 0.005 to 0.50% V, 0.005 to 0.20% Nb, 0.003 to 0.050% Al, and 0.003 to 0.050% Ti, and further simultaneously comprising ≥0.0001% Mg and Ca respectively, and in which the total lies in the range of 0.0010 to 0.010%, and the balance iron with inevitable impurities, and the content of the Mg has the relation expressed by formula {free [Mg]=total [Mg]-[Mg] contained in the total oxide≥1 ppm}.;COPYRIGHT: (C)2008,JPO&INPIT
机译:解决的问题:提供一种在超高热输入焊接部件HAZ(热影响区)中具有优异韧性的高强度焊接结构用钢,并提供其生产方法。在超高热输入焊接部件中具有出色的韧性HAZ的成分包括以质量%计的0.01至0.20%C,0.02至0.50%Si,1.5至3.5%Mn,≤0.03%P,0.005至0.030%S,0.005至0.50%的V,0.005至0.20%的Nb,0.003至0.050%的Al和0.003至0.050%的Ti,并且进一步同时分别包含≥0.0001%的Mg和Ca,并且其总量在0.0010至0.010的范围内%,余量的铁具有不可避免的杂质,并且Mg的含量具有由式{游离的[Mg] =总的[Mg]-[Mg]包含在总氧化物中≥ 1 ppm}表示的关系。COPYRIGHT:( C)2008,日本特许厅

著录项

  • 公开/公告号JP5245202B2

    专利类型

  • 公开/公告日2013-07-24

    原文格式PDF

  • 申请/专利权人 新日鐵住金株式会社;

    申请/专利号JP20060083017

  • 发明设计人 福永 和洋;渡部 義之;植森 龍治;

    申请日2006-03-24

  • 分类号C22C38/00;C22C38/14;C22C38/58;C21D8/02;

  • 国家 JP

  • 入库时间 2022-08-21 16:57:25

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号