An atmospheric leach process in the recovery of nickel and cobalt from lateritic ores, said processing including the steps of: a) separating the lateritic ore into a low magnesium containing ore fraction, and a high magnesium containing ore fraction by selective mining or post mining classification; b) separately slurrying the separated ore fractions; c) leaching the low magnesium containing ore fraction with concentrated sulphuric acid as a primary leach step; and d) introducing the high magnesium content ore slurry following substantial completion of the primary leach step and precipitating iron as goethite or another low sulphate containing form of iron oxide or iron hydroxide, wherein sulphuric acid released during iron precipitation is used to leach the high magnesium ore fraction as a secondary leach step.
机译:从红土矿石中回收镍和钴的常压浸出工艺,所述处理包括以下步骤:a)通过选择性采矿或后采矿分类将红土矿石分离为低镁含量的矿石级分和高镁含量的矿石级分; b)分别将分离出的矿石级分浆化; c)作为主要的浸出步骤,用浓硫酸浸出低镁的矿石部分; d)在基本浸出步骤基本完成之后引入高镁含量的矿浆,并沉淀铁为针铁矿或另一种低硫酸盐形式的氧化铁或氢氧化铁,其中铁沉淀过程中释放出的硫酸用于浸出高镁矿石级分作为二级浸出步骤。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号