PROBLEM TO BE SOLVED: To provide a method for treating a seam part slab with which the length of component mixing region of succeeding charge can concretely be obtained by using a calculating formula when sequentially casting different steels.;SOLUTION: When performing the continuous casting by pouring the molten steels different in components into a tundish remaining a preceding molten steel as the succeeding charge, the slab position corresponding to the molten steel surface position at the time point of pouring the succeeding charge into the tundish is defined as a basic position, and the slab of the succeeding charge up to the range of the slab length (L) calculated with a (1) formula from the basic position is treated as scrap. Wherein, in the (1) formula of L=(a×WTD+b)/(SST×ρ)+c, L is the slab length (m); WTD is the remained molten steel quantity (ton) in the tundish at the time point of starting the pouring of the following successive molten steel; SST is the total value (m2) of the cross sectional area of the slab; ρ is density (ton/m3) of the slab; a, b, c are independently factors; and they are preferrably set to a=1.39, b=0 and c=0.8.;COPYRIGHT: (C)2009,JPO&INPIT
机译:解决的问题:提供一种用于处理接缝部分坯的方法,利用该方法可以在依次浇铸不同的钢时通过使用计算公式来具体地获得后续装料的组分混合区域的长度。将成分不同的钢水倒入中间包而保留之前的钢水作为后续进料,将与随后的进料倒入中间包时的钢水表面位置相对应的板坯位置定义为基本位置,并且从基本位置开始,用(1)式计算出的板坯长度(L)以内的后续装料板坯视为废料。其中,在L =(a× W TD + b)/(S ST ρ)+ c的(1)公式中,L为板坯长度(m); W TD 是开始浇铸后续连续钢水时中间包中的剩余钢水量(吨); S ST 是平板横截面的总和(m 2 ); ρ是板的密度(吨/米 3 ); a,b,c是独立因素;并且最好将它们设置为a = 1.39,b = 0和c = 0.8。; COPYRIGHT:(C)2009,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号