首页> 外国专利> Phosphorus recovery materials and phosphorus recovery process

Phosphorus recovery materials and phosphorus recovery process

机译:磷回收材料及磷回收工艺

摘要

PPROBLEM TO BE SOLVED: To provide a phosphorus recovery material and method which do not require a large apparatus when recovering phosphorus from wastewater or the like, and allow the recovered material to be used as a by-product phosphate fertilizer. PSOLUTION: The phosphorus recovery material is used for coagulating sedimentation, and is made of a porous calcium silicate hydrate which is a fine powder having an average particle size (a median diameter) of 150 μm or less, and has a pore volume of 0.3 cmSP3/SP/g or more, preferably, the calcium silicate hydrate having an average particle size of 10 μm or more and 150 μm or less, a bulk density of 0.1 g/cmSP3/SPor more and 0.7 g/cmSP3/SPor less, and a Ca/Si molar ratio of 0.4 or more and 1.5 or less. In the phosphorus recovery method, an acid is added, calcium is eluted by sequential decomposition of the calcium silicate hydrate to generate hydroxyapatite on the surface of the calcium silicate hydrate particles, and the coagulated precipitate is separated to recover phosphorus. PCOPYRIGHT: (C)2010,JPO&INPIT
机译:

要解决的问题:提供一种从废水等中回收磷时不需要大型设备的磷回收材料和方法,并使回收的材料用作副产品磷酸盐肥料。

解决方案:磷回收材料用于凝结沉淀,由多孔硅酸钙水合物制成,该多孔硅酸钙水合物是平均粒径(中值直径)为150μm或更小的细粉。孔体积为0.3cm 3 / g以上,优选平均粒径为10μm以上且150μm以下,堆积密度为0.1g的硅酸钙水合物/ cm 3 以上且0.7 g / cm 3 以下,且Ca / Si摩尔比为0.4以上且1.5以下。在磷回收方法中,添加酸,通过依次分解水合硅酸钙来洗脱钙以在水合硅酸钙颗粒的表面上生成羟基磷灰石,并且将凝结的沉淀物分离以回收磷。

版权:(C)2010,日本特许厅&INPIT

著录项

  • 公开/公告号JP5201454B2

    专利类型

  • 公开/公告日2013-06-05

    原文格式PDF

  • 申请/专利权人 小野田化学工業株式会社;

    申请/专利号JP20080143895

  • 发明设计人 美濃和 信孝;

    申请日2008-05-30

  • 分类号C02F1/58;C01B33/24;B01D21/01;C05B7/00;C05F7/00;C05G3/00;

  • 国家 JP