It consists of the calcination preprocessing manner of the honeycomb compact and the calcination preprocessing system null ceramic

机译:它由蜂窝坯的煅烧预处理方式和煅烧预处理体系组成。

摘要

PROBLEM TO BE SOLVED: To provide a method of firing pre-treating a honeycomb formed body by which the honeycomb formed body is firing pre-treated for a short time while suppressing the occurrence of failure such as deformation or breaking.;SOLUTION: The method of firing pre-treating an un-fired honeycomb formed body 1 which comprise a raw material composition containing a ceramic raw material, water and a binder and has a plurality of cells divided by partitions to form a flow passage of a fluid has a first step for passing superheated steam of 100-150°C through the cells to raise the temperature of the honeycomb formed body and after that, keeping the honeycomb formed body at the temperature of the superheated steam ranging from equal to or above the temperature of the steam passed through the cells to ≤200°C and a second step for keeping the honeycomb formed body at the temperature of a superheated steam atmosphere ranging from equal to or above the temperature in the first step to ≤600°C after the first step.;COPYRIGHT: (C)2008,JPO&INPIT
机译:解决的问题:提供一种对蜂窝成形体进行预烧成的方法,通过该方法对蜂窝成形体进行短时间的预烧成,同时抑制诸如变形或破裂等故障的发生。焙烧预处理未焙烧的蜂窝成形体1的步骤,该第一步包括:含有陶瓷原料,水和粘合剂的原料组合物,并具有多个被分隔壁隔开的小室,以形成流体的流动通道。用于使100-1500℃的过热蒸汽通过小室以升高蜂窝成形体的温度,然后,使蜂窝成形体保持在等于或高于所通过的蒸汽温度的过热蒸汽的温度下通过小室至约200℃,以及第二步骤,以将蜂窝成形体保持在等于或高于冷杉温度的过热蒸汽气氛的温度下。第一步后,温度升至600摄氏度。;版权:(C)2008,JPO&INPIT

著录项

  • 公开/公告号JP5108277B2

    专利类型

  • 公开/公告日2012-12-26

    原文格式PDF

  • 申请/专利权人 日本碍子株式会社;

    申请/专利号JP20060296233

  • 发明设计人 櫻井 隆行;林 伸三;

    申请日2006-10-31

  • 分类号C04B35/638;B28B11/00;

  • 国家 JP

  • 入库时间 2022-08-21 16:54:12