首页> 外国专利> Be sure to grind in the form which makes the continuous casting throb of the production mannered null CrNi rustless steel of the CrNi

Be sure to grind in the form which makes the continuous casting throb of the production mannered null CrNi rustless steel of the CrNi

机译:确保以一定的形式研磨,使连续铸造的CrNi原始CrNi无锈钢成为不锈钢

摘要

PROBLEM TO BE SOLVED: To provide a manufacturing method which can stably suppress the occurrence of edge cracks of a Cr-Ni-based stainless steel strip caused during hot rolling.;SOLUTION: After grinding a continuously cast slab into a shape in which the thicknesses in width end parts are thickened as compared with that in the middle part of the width, when making the ground slab into a hot-rolled steel strip by performing hot rolling in a process of (heating-rough rolling-finish rolling), the rolling in the width direction is definitely performed by odd numbered pass in the rough rolling and is performed at the edging quantity in rolling of the width direction, which is defined by the next formula (1), of ≥7 mm in any pass.;COPYRIGHT: (C)2010,JPO&INPIT
机译:要解决的问题:提供一种能够稳定地抑制在热轧过程中引起的Cr-Ni基不锈钢带材边缘裂纹的发生的方法;解决方案:将连续铸造的板坯研磨成一定厚度后的形状与在宽度的中间部分相比,在宽度方向上的端部加厚,当在(加热粗轧-终轧)过程中通过进行热轧将板坯制成热轧钢带时,沿宽度方向的轧制肯定是通过粗轧中的奇数道次进行的,并且在宽度方向的轧制中由下一个公式(1)定义的磨边量在任何道次中都为≥7mm。版权:(C)2010,日本特许厅和INPIT

著录项

  • 公开/公告号JP5152791B2

    专利类型

  • 公开/公告日2013-02-27

    原文格式PDF

  • 申请/专利权人 日新製鋼株式会社;

    申请/专利号JP20080063958

  • 发明设计人 香月 淳一;相沢 敦;広田 龍二;

    申请日2008-03-13

  • 分类号B21B1/02;B21B3/02;

  • 国家 JP

  • 入库时间 2022-08-21 16:53:58