Provided is a process for producing a polyether polyol which can form low viscosity rigid foamed synthetic resins excellent in strength, dimensional stability and flame retardancy, can give a low viscosity polyol system solution containing water instead of HFCs as a blowing agent with good miscibility with isocyanate compounds and can form good rigid foamed synthetic resins by spraying. A polyether polyol (A) is produced by reacting a phenol component (molar ratio 1) selected from phenol and phenol derivatives having a hydrogen atom at one or more ortho-positions to the phenolic hydroxyl group, an aldehyde component (molar ratio 0.3 to 0.9) selected from formaldehyde and acetoaldehyde and an alkanolamine component (molar ratio 1.5 to 3.5) selected from monoethanolamine, diethanolamine and 1-amino- 2-propanol and then adding an alkylene oxide to the resulting reaction product.
机译:提供了一种制备聚醚多元醇的方法,该聚醚多元醇可以形成强度,尺寸稳定性和阻燃性优异的低粘度硬质泡沫合成树脂,可以提供一种低粘度的多元醇体系溶液,该溶液含有水而不是HFC作为发泡剂,并与异氰酸酯具有良好的混溶性。可以通过喷涂形成良好的硬质泡沫合成树脂。聚醚多元醇(A)是通过使选自酚和在一个或多个邻位具有氢原子的酚衍生物的酚成分(摩尔比为1)与酚羟基,醛成分(摩尔比为0.3〜0.9)反应而制备的。 )选自甲醛和乙醛)和选自单乙醇胺,二乙醇胺和1-氨基-2-丙醇的链烷醇胺组分(摩尔比为1.5至3.5),然后将环氧烷加入到所得反应产物中。

著录项

  • 公开/公告号IN2011CN09053A

    专利类型

  • 公开/公告日2013-05-24

    原文格式PDF

  • 申请/专利权人

    申请/专利号IN9053/CHENP/2011

  • 申请日2011-12-05

  • 分类号C08G14/12;C08L75/08;C08J9/04;C07C213/06;C08J9/08;C08J9/35;C08G101/00;C08G18/63;C08G18/48;C07C213/00;C08G18/50;C08G18/54;C07C215/10;C08G18/00;C08G65/28;

  • 国家 IN

  • 入库时间 2022-08-21 16:41:21

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号