An austenitic stainless steel welded joint, which comprises by mass%, C: 0.05 to 0.25%, Si: not more than 2%, Mn: 0.01 to 3%, P: 0.05 to 0.5%, S: not more than 0.03%, Cr: 15 to 30%, Ni: 6 to 55%, sol. Al: 0.001 to 0.1% and N: not more than 0.03%, with the balance being Fe and impurities, and satisfies the formula of (Cr + 1.5 × Si + 2 × P)/(Ni + 0.31 × Mn + 22 × + 14.2 × N + 5 × P) ≥ 1.388, has high creep strength, and moreover, is economical and excellent in weldability. Therefore, the said austenitic stainless steel welded joint can be widely applied as steel pipes, steel plates and so on in such fields where not only high-temperature strength and corrosion resistance but also weldability is required. Each element symbol in the above formula represents the content by mass percent of the element concerned.
机译:奥氏体不锈钢焊接接头,以质量%计,C:0.05〜0.25%,Si:2%以下,Mn:0.01〜3%,P:0.05〜0.5%,S:0.03%以下, Cr:15至30%,Ni:6至55%,溶胶。 Al:0.001〜0.1%,N:0.03%以下,其余为Fe和杂质,满足(Cr + 1.5×Si + 2×P)/(Ni + 0.31×Mn + 22×​​+ 14.2×N + 5×P)≥1.388,蠕变强度高,而且经济且焊接性优异。因此,上述奥氏体系不锈钢焊接接头可广泛用于不仅要求高温强度和耐腐蚀性还要求可焊接性的领域中的钢管,钢板等。上式中的每个元素符号表示有关元素的质量百分比。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号