PURPOSE: A manufacturing method of semi-crystalline and semi-aromatic copolyamide is provided to improve reaction rate of chain extending reaction and to obtain semi-crystalline and semi-aromatic copolyamide with extremely high molecular weight within very short reaction time.;CONSTITUTION: A manufacturing method of semi-crystalline and semi-aromatic copolyamide comprises: a step of preparing a copolyamide prepolymer comprising an aromatic dicarboxylic acid, aromatic dicarboxylic acid and aliphatic diamine; and a step of increasing the molecular weight of the copolyamide prepolymer through a solid polymerization. The relative viscosity of the copolyamide prepolymer is 1.05 or more. The aromatic dicarboxylic acid is at least one selected from terephthalic acid and isophthalic acid.;COPYRIGHT KIPO 2013
机译:目的:提供一种半结晶和半芳香族共聚酰胺的制备方法,以提高扩链反应的反应速率,并在很短的反应时间内获得分子量极高的半结晶和半芳香族共聚酰胺。半结晶半芳族共聚酰胺的制造方法包括:制备包含芳族二羧酸,芳族二羧酸和脂肪族二胺的共聚酰胺预聚物的步骤;通过固相聚合来提高共聚酰胺预聚物的分子量的步骤。共聚酰胺预聚物的相对粘度为1.05以上。芳族二羧酸是选自对苯二甲酸和间苯二甲酸中的至少一种。; COPYRIGHT KIPO 2013

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号