HIGH EXCLAMATION MACROMOLECULES SUPPORT AND MANUFACTURING METHOD THEREOF, STRUCTURE OF MACROMOLECULES SUPPORT-CHONDROCYTE COMPLEX BASED ON THE SAME, AND CHONDROCYTE RESTRUCTURING METHOD USING THE SAME

机译:高度抗微生物大分子支持及其制备方法,基于相同分子的大分子支持-软骨细胞复合物的结构以及使用相同方法的软骨细胞重组方法

摘要

PURPOSE: A high elastic polymer supporter, a manufacturing method thereof, a polymer support - chondrocyte compound structure based on the same, and a cartilage reconstruction method are provided to enhance recovery properties and bio compatibility. CONSTITUTION: A high elastic polymer supporter is manufactured with blending composition in which poly octyl cyano acrylate and poly-e-caprolactone are blended at the fixed rate. The poly octyl cyano acrylate has the weight-average molecular weight of 50,000 - 500,000. The poly-e-caprolactone has the weight-average molecular weight of 60,000-80,000. The molar ratio of the poly octyl cyano acrylate of the poly octyl cyano acrylate and poly-e-caprolactone blending supporter is in 30 - 70% range. [Reference numerals] (AA) Recovery rate(%); (BB) 4:6 recovery rate(%); (CC) 5:5 recovery rate(%); (DD) 6:4 recovery rate(%); (EE) Deformation rate(%)
机译:目的:提供一种高弹性的聚合物载体,其制造方法,基于该聚合物载体的软骨细胞复合结构以及一种软骨重建方法,以增强恢复性能和生物相容性。组成:一种高弹性聚合物载体,其制备方法是将氰基丙烯酸聚辛酯和ε-己内酯按固定比例混合。聚氰基丙烯酸辛基酯的重均分子量为50,000-500,000。聚-ε-己内酯的重均分子量为60,000-80,000。聚氰基丙烯酸辛酯和聚ε-己内酯混合载体中的聚氰基丙烯酸辛酯的摩尔比在30〜70%的范围内。 [参考数字](AA)回收率(%); (BB)4:6回收率(%); (CC)5:5回收率(%); (DD)6:4回收率(%); (EE)变形率(%)

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号