PURPOSE: A method for controlling welding defects by reducing aluminum-silicon-magnesium alloy particle size and improving cooling rate is provided to minimize the size of a needle-shaped insertion phase and reduce the amount of the needle-shaped insertion phase in welding. CONSTITUTION: A method for controlling welding defects reduces the particle size of Al-Si-Mg alloy and improves cooling rate by electromagnetic pulse treatment which removes welding defect of Al-Si-Mg alloy by irradiating the Al-Si-Mg alloy with the electromagnetic pulse form an electromagnetic pulse generators. The electromagnetic pulse generator which comprises a wave guide for transferring the electromagnetic pulse to the inside of a weld can reduce the size of the Al-Si-Mg alloy particle and improves cooling rate. The material of the wave guide is titanium material. The wave guide is located in the inside of the weld. The Al-Si-Mg alloy is an Al-6-7 wt% of Si-Mg alloy which is a 356 or 357 alloy. [Reference numerals] (AA) Untreated with electromagnetic pulses; (BB) Treated with electromagnetic pulses of 2Hz; (CC) Treated with electromagnetic pulses of 4Hz; (DD) Treated with electromagnetic pulses of 6Hz
机译:目的:提供一种通过减小铝硅镁合金颗粒尺寸并提高冷却速率来控制焊接缺陷的方法,以最小化针形插入相的尺寸并减少焊接中针形插入相的数量。组成:一种控制焊接缺陷的方法,通过电磁脉冲处理可减小Al-Si-Mg合金的粒径并提高冷却速度,该电磁脉冲处理可通过用电磁辐射对Al-Si-Mg合金进行辐照来消除Al-Si-Mg合金的焊接缺陷。脉冲形成电磁脉冲发生器。包括用于将电磁脉冲传递到焊缝内部的波导的电磁脉冲发生器可以减小Al-Si-Mg合金颗粒的尺寸并提高冷却速度。波导的材料是钛材料。波导位于焊缝内部。 Al-Si-Mg合金是Si-Mg合金的Al-6-7重量%,Si-Mg合金是356或357合金。 [附图标记](AA)未经电磁脉冲处理; (BB)用2Hz的电磁脉冲处理; (CC)用4Hz电磁脉冲处理; (DD)经过6Hz电磁脉冲处理

著录项

  • 公开/公告号KR20130011208A

    专利类型

  • 公开/公告日2013-01-30

    原文格式PDF

  • 申请/专利权人 KOREA INSTITUTE OF MACHINERY & MATERIALS;

    申请/专利号KR20110072193

  • 发明设计人 KIM KYUNG HYUN;

    申请日2011-07-21

  • 分类号B22D27/02;C22B9/02;C22C1/02;

  • 国家 KR

  • 入库时间 2022-08-21 16:27:47

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号