PURPOSE: A manufacturing method of an amphiphilic block copolymer is provided to simplify synthesis of a RAFT polymerization method which can accurately control molecular weight without a metallic catalyst, and to obtain uniform size distribution.;CONSTITUTION: An amphiphilic block copolymer comprises polyester as a hydrophobic block, and polyphosphoryl choline as a hydrophilic block. A manufacturing method of the amphiphilic block copolymer comprises: a step of polymerizing a polyester block through ring-opening polymerization; a step of adding a chain-moving reactant into the polyester block; and a step of adding phosphoryl choline into the polyester block, and polymerizing a polyester-polyphosphoryl chlorine block copolymer by a living radical method.;COPYRIGHT KIPO 2013
机译:目的:提供一种两亲嵌段共聚物的制造方法,以简化RAFT聚合方法的合成,该方法无需金属催化剂即可精确控制分子量,并获得均匀的尺寸分布。;组成:两亲嵌段共聚物包含聚酯作为疏水性嵌段和多磷酰胆碱作为亲水性嵌段。所述两亲性嵌段共聚物的制造方法包括:通过开环聚合使聚酯嵌段聚合的步骤;向聚酯嵌段中加入链转移反应物的步骤;以及将磷酰胆碱加入到聚酯嵌段中,并通过活性自由基法聚合聚酯-聚磷酰氯嵌段共聚物的步骤。; COPYRIGHT KIPO 2013

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号