PURPOSE: A continuous manufacturing method of a ferritic stainless steel is provided to improve a surface quality degradation of a stainless steel due to a roping bending after a continuous cold rolling by gradually reducing a roll illumination of a rolling mill used in the continuous cold rolling.;CONSTITUTION: A continuous manufacturing method of a ferritic stainless steel comprises the following steps: a stainless steel is rolled by a continuous rolling mill equipped with more than two rolling mill stands; and a stainless steel going through a continuous rolling step is rolled by a reversible mill. The stainless steel is rolled to a gradually reduced roll illumination in a rolling mill stand having a roll illumination of less than 1.5μm and more than 0.2μm in the continuous rolling step. In the continuous rolling mill, a roll illumination of a first rolling mill stand is more than 1.0μm less than 1.5μm, a roll illumination of a second and third rolling mill stand is more than 0.4μm less than 0.8μm, and a roll illumination of a fourth rolling mill stand is more than 0.2μm less than 0.4μm.;COPYRIGHT KIPO 2013;[Reference numerals] (AA) Oil pit area ratio(%); (BB) Comparative example 1; (CC) Comparative example 2; (DD) Comparative example 3; (EE) Example 1; (FF) Example 2
机译:用途:提供一种铁素体不锈钢的连续制造方法,以通过逐渐减少连续冷轧中使用的轧机的辊照度来改善由于连续冷轧后的翘曲弯曲而引起的不锈钢的表面质量劣化。组成:铁素体不锈钢的连续制造方法包括以下步骤:用配备有两个以上轧机机架的连续轧机轧制不锈钢;然后,通过可逆轧机将经过连续轧制步骤的不锈钢轧制。在连续轧制步骤中,在轧制照度小于1.5μm且大于0.2μm的轧机机架中将不锈钢轧制至逐渐降低的轧制照度。在连续轧机中,第一轧机机架的轧辊照度大于1.0μm小于1.5μm,第二和第三轧机机架的轧辊照度大于0.4μm小于0.8。 ,并且第四轧机机架的辊照明度大于0.4μm,小于0.2μm; COPYRIGHT KIPO 2013; [参考数字](AA)油坑面积比(%); (BB)比较例1; (CC)比较例2; (DD)比较例3; (EE)示例1; (FF)示例2

著录项

  • 公开/公告号KR20130055909A

    专利类型

  • 公开/公告日2013-05-29

    原文格式PDF

  • 申请/专利权人 POSCO;

    申请/专利号KR20110121580

  • 发明设计人 OH TAEG SU;KIM CHUL HEE;KIM JIN SUK;

    申请日2011-11-21

  • 分类号B21B1/24;B21B3/02;B21B1/32;C22C38/18;

  • 国家 KR