首页> 外国专利> METHOD FOR PRODUCING SOL-GEL DERIVED POROUS, BIOACTIVE GLASS MICROSPHERES USING CHITOSAN AS BIOMOLECULAR TEMPLATE AND THEREOF

METHOD FOR PRODUCING SOL-GEL DERIVED POROUS, BIOACTIVE GLASS MICROSPHERES USING CHITOSAN AS BIOMOLECULAR TEMPLATE AND THEREOF

机译:以壳聚糖为生物分子模板制备溶胶-凝胶衍生的多孔生物玻璃微球的方法及其方法

摘要

PURPOSE: A multi porous bioactive spherical particle manufactured by using chitosan as a template is provided to be used in various fields such as a medicine transfer system or a reinforcement purpose of a biodegradable polymer, etc. as the particle has porosity. CONSTITUTION: A production method of a multi porous bioactive spherical particle includes the production of bioactive glass sol mixed with a chitosan solution and bioactive glass, and a process of making the bioactive glass sol into gel before treating with heat. The chitosan solution further includes acetic acid. The pH of the chitosan solution is 2-3. The bioactive glass includes a mixture of tetraethyl orthosilicate, triethylphosphate, and calcium nitrate. A mole fraction of a silicon oxide, a calcium oxide, and phosphorus pentoxide in the bioactive glass sol is 60:25:15 to 60:39:1. A gelation process is performed for 6-10 hours at a range of 50-70 deg. C. [Reference numerals] (AA) Chitosan particle treated to have positive potential; (BB) Coagulation of bioactive glass particle; (CC) Self assembly of chitosan-bioactive glass complex; (DD) Spherical micro particle with nano pores
机译:目的:提供一种以壳聚糖为模板制备的多孔生物活性球形颗粒,由于该颗粒具有孔隙率,因此可用于各种领域,例如药物转移系统或可生物降解聚合物的增强目的等。组成:多孔生物活性球形颗粒的生产方法包括混合壳聚糖溶液和生物活性玻璃的生物活性玻璃溶胶的生产,以及在加热处理之前将生物活性玻璃溶胶制成凝胶的过程。壳聚糖溶液还包含乙酸。壳聚糖溶液的pH为2-3。生物活性玻璃包括原硅酸四乙酯,磷酸三乙酯和硝酸钙的混合物。生物活性玻璃溶胶中的氧化硅,氧化钙和五氧化二磷的摩尔分数为60:25:15至60:39:1。在50-70度的范围内进行胶凝过程6-10小时。 C. [参考数字](AA)被处理为具有正电势的壳聚糖颗粒; (BB)生物活性玻璃颗粒的凝结; (CC)壳聚糖-生物活性玻璃复合物的自组装; (DD)具有纳米孔的球形微粒

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号