首页> 外国专利> ELECTRICAL PHOTOGRAPHIC PHOTOSENSITIVE MATERIAL WITH EXCELLENT LIFETIME PROTERTY AND ELECTRIFICATION HOMOGENIETY OBTAINING EXCELLENT PICTURE QUALITY FOR LONG TIME, AND ELECTRIC PHOTOGRAPHIC IMAGE FORMING APPARATUS AND ELECTROPHOTOGRAPHY CARTRIDGE ADOPTING THE SAME

ELECTRICAL PHOTOGRAPHIC PHOTOSENSITIVE MATERIAL WITH EXCELLENT LIFETIME PROTERTY AND ELECTRIFICATION HOMOGENIETY OBTAINING EXCELLENT PICTURE QUALITY FOR LONG TIME, AND ELECTRIC PHOTOGRAPHIC IMAGE FORMING APPARATUS AND ELECTROPHOTOGRAPHY CARTRIDGE ADOPTING THE SAME

机译:长期具有优异图像质量的,具有优异寿命和电气均质性的光电照相材料,以及采用该光电照相图像形成装置和电子照相仪

摘要

PURPOSE: An electrical photographic photosensitive material is provided to have excellent electric charge smudge property even when thick charge transport layer is adopted by improving the response speed.;CONSTITUTION: A stack electrical photographic photosensitive material comprises an electrical conductive support, an undercoat layer, a charge generating layer and a charge transporting layer. The characteristic response time of photosensitive material is more than 10msec and less than 85msec, and the thickness of the charge transport layer of the photosensitive material is 18micrometers to 45 micrometers. The characteristic response time is defined as the shorted response time in rage between specific photoinduction discharge curve(PIDC) produced response time. The response time is defined as the elapsed time from the stack electrical photographic layer applied on exposure to the time applied on the phenomenon. The charge generation layer comprises phthalocyanine compound charge generation material and binder in 1:0.3-1:4 weight ratio. The charge transport layer comprises the charge transfer material and binger in 1:0.5-1:2 weight ratio.;COPYRIGHT KIPO 2013;[Reference numerals] (AA) Surface potential Vo (V); (BB) Time(sec)
机译:用途:提供一种电子照相感光材料,即使通过提高响应速度采用厚的电荷传输层,也具有优异的电荷污染性能;组成:堆叠式电子照相感光材料包括导电载体,底涂层,电荷产生层和电荷传输层。感光材料的特征响应时间大于10毫秒且小于85毫秒,并且感光材料的电荷传输层的厚度为18微米至45微米。特征响应时间定义为特定光感应放电曲线(PIDC)产生的响应时间之间的较短响应时间。响应时间定义为从曝光时施加的电子照相叠层到现象发生时所经过的时间。电荷产生层包括重量比为1:0.3-1:4的酞菁化合物电荷产生材料和粘合剂。电荷传输层包括重量比为1:0.5-1:2的电荷转移材料和粘合剂。; COPYRIGHT KIPO 2013; [参考数字](AA)表面电势Vo(V); (BB)时间(秒)

著录项

  • 公开/公告号KR20130067664A

    专利类型

  • 公开/公告日2013-06-25

    原文格式PDF

  • 申请/专利权人 SAMSUNG ELECTRONICS CO. LTD.;

    申请/专利号KR20110134460

  • 发明设计人 KIM JI UK;

    申请日2011-12-14

  • 分类号G03G5/04;G03G5/047;G03G5/147;G03G15/02;