PURPOSE: A polycarbonate resin composition is provided to apply in the parts of electronic products as the composition has heat resistance, flame resistance, scratch resistacne, mechanical property and transparency.;CONSTITUTION: A scratch resistant polycarbonate resin composition contains (A) 50-99 weight% of polycarbonate resin; (B) 1-50 weight% of (meth)acrylic copolymer containing a biphenyl group with 1.495-1.640 of refractive index; (C) 0-30 parts by weight of a rubber-modified vinyl graft copolymer resin; and (D) 0-30 parts by weight of phosphoric flame retardant per 100.0 parts by weight of the polycarbonate resin composition. The (meth)acrylate copolymer(B) has a glass transition temperature ranged 90-150 degreeC and a weight average molecular weight ranged 3,000-300,000.;COPYRIGHT KIPO 2013
机译:用途:提供一种聚碳酸酯树脂组合物,因为该组合物具有耐热性,阻燃性,抗划痕性痤疮,机械性能和透明性,因此可用于电子产品的组成部分;;组成:一种抗划伤性聚碳酸酯树脂组合物,其中包含(A)50-99聚碳酸酯树脂的重量%; (B)1-50重量%的具有联苯的,折射率为1.495-1.640的(甲基)丙烯酸共聚物; (C)0-30重量份的橡胶改性的乙烯基接枝共聚物树脂; (D)相对于100.0重量份的聚碳酸酯树脂组合物为0〜30重量份的磷系阻燃剂。 (甲基)丙烯酸酯共聚物(B)的玻璃化转变温度为90-150℃,重均分子量为3,000-300,000。; COPYRIGHT KIPO 2013

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号