首页> 外国专利> Iron-cobalt catalyst, manufacturing method same and method for obtaining water-gas shift reaction activity and for highly selective liquid fuel production in Fischer-Tropsch synthesis using iron-cobalt catalyst

Iron-cobalt catalyst, manufacturing method same and method for obtaining water-gas shift reaction activity and for highly selective liquid fuel production in Fischer-Tropsch synthesis using iron-cobalt catalyst

机译:铁钴催化剂,其制造方法以及在使用铁钴催化剂进行的费托合成中获得水煤气变换反应活性和高选择性液体燃料生产的方法

摘要

PURPOSE: A method for preparing iron-cobalt composite catalyst and a method for implementing water-gas shift reaction activity in Fischer-Tropsch synthesis and producing highly selective liquid fuel using the same are provided to enhance the yield of liquid. CONSTITUTION: A method for preparing iron-cobalt composite catalyst comprises: a step of supporting 5-20 parts by weight of cobalt with respect to 100 parts by weight of an iron catalyst(S140); and drying the supported iron-cobalt at 100-150 deg.C. for 3-5 hours(S150). The method further comprises a step of plasticizing the iron-coba and a step of reducing the iron-cobalt under a hydrogen atmosphere. [Reference numerals] (AA) Start; (BB) End; (S100) Precipitating iron(Fe), copper(Cu), and Na_2CO_3; (S110) Washing for removing sodium elements from precipitate; (S120) Mixing an SiO_2 solution and a K_2CO_3 solution with the precipitate; (S130) Spray-drying; (S140) Supporting the predetermined amount of coba (S150) Drying the supported iron-cobalt
机译:目的:提供一种用于制备铁-钴复合催化剂的方法和在费-托合成中实现水煤气变换反应活性并使用该方法生产高选择性液体燃料的方法,以提高液体的产率。组成:一种铁钴复合催化剂的制备方法,包括:相对于100重量份的铁催化剂负载5-20重量份的钴的步骤(S140);并在100-150℃下干燥负载的铁钴。持续3-5个小时(S150)。该方法还包括增塑铁-钴的步骤;在氢气氛下还原铁钴的步骤。 [参考数字](AA)开始; (BB)结束; (S100)沉淀出铁(Fe),铜(Cu)和Na_2CO_3; (S110)洗涤以去除沉淀物中的钠元素; (S120)将SiO_2溶液和K_2CO_3溶液与沉淀物混合; (S130)喷雾干燥; (S140)支撑预定量的钴; (S150)干燥支撑的铁钴

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号