首页> 外国专利> HIGH CARBON FORGING WORK ROLL FOR HOT ROLLING HAVING AN EXCELLENT HIGH TEMPERATURE WEAR RESISTANCE AND MECHANICAL STRENGTH AND A MANUFACTURING METHOD THEREOF CAPABLE OF MANUFACTURING THE SAME THROUGH A STEP OF HOT FORGING AND A STEP OF A HEAT TREATMENT

HIGH CARBON FORGING WORK ROLL FOR HOT ROLLING HAVING AN EXCELLENT HIGH TEMPERATURE WEAR RESISTANCE AND MECHANICAL STRENGTH AND A MANUFACTURING METHOD THEREOF CAPABLE OF MANUFACTURING THE SAME THROUGH A STEP OF HOT FORGING AND A STEP OF A HEAT TREATMENT

机译:具有出色的高温耐磨性和机械强度的热轧高碳锻造轧制工装,其制造方法可通过热锻造和热处理来实现

摘要

PURPOSE: A high carbon forging work roll for hot rolling having an excellent wear resistance at high temperature and mechanical strength and a manufacturing method thereof are provided to implement a step of hot forging and a step of a heat treatment on the work roll at an optimal temperature range, thereby providing the high wear resistance at the high temperature to the work roll.;CONSTITUTION: A manufacturing method of a high carbon forging work roll for hot rolling having an excellent wear resistance at high temperature and mechanical strength includes: a step of manufacturing an ingot; a hot forging step of forming the work roll with heating and forging the ingot in a heating furnace; and a heat treatment step of heat-treating the work roll with passing the work roll through a step of normalizing, a step of forcible cooling, and a step of tempering. The hot forging step includes: an initial hot forging step of sequentially implementing an upsetting process and a cogging process at a temperature of 950 to 1200°C; and a final hot forging step of implementing a finishing process at a temperature of 700 to 950°C.;COPYRIGHT KIPO 2013;[Reference numerals] (AA) Start; (BB) End; (S100) Ingot manufacturing step; (S200) Work roll heating and forging step; (S300) Heat-treating step
机译:目的:提供一种在高温下具有优异的耐磨性和机械强度的用于热轧的高碳锻造工作辊及其制造方法,以在工作辊上以最佳方式实施热锻造步骤和热处理步骤。组成:一种用于高温轧制的高碳锻造工作辊的制造方法,该方法在高温下具有优异的耐磨性和机械强度,该方法包括以下步骤:制造锭;热锻工序,其通过加热形成工作辊并在加热炉中锻造铸锭;热处理步骤是使工作辊通过正火化步骤,强制冷却步骤和回火步骤而对工作辊进行热处理的步骤。热锻步骤包括:初始热锻步骤,其依次在950至1200°C的温度下进行up锻工艺和嵌齿工艺。最终的热锻步骤是在700至950℃的温度下进行精加工; COPYRIGHT KIPO 2013; [附图标记](AA)开始; (BB)结束; (S100)铸锭制造步骤; (S200)工作辊加热锻造步骤; (S300)热处理步骤

著录项

  • 公开/公告号KR101286121B1

    专利类型

  • 公开/公告日2013-07-17

    原文格式PDF

  • 申请/专利权人 SEOHAN INDUSTRY CO. LTD.;

    申请/专利号KR20120157801

  • 发明设计人 MIN KYU YOUNG;KWON MIN KI;PARK YOUNG TAE;

    申请日2012-12-31

  • 分类号B21K1/02;B21K21/00;B21J5/08;C22C38/00;

  • 国家 KR