首页> 外国专利> FIRMING COMPOSITION FOR HARDENING WEAK GROUND USING EARLY-STRENGTH CEMENT AND INDUSTRIAL BY-PRODUCT OF MINERALS AND THE MANUFACTURING METHOD THEREOF

FIRMING COMPOSITION FOR HARDENING WEAK GROUND USING EARLY-STRENGTH CEMENT AND INDUSTRIAL BY-PRODUCT OF MINERALS AND THE MANUFACTURING METHOD THEREOF

机译:利用矿物质的早期强度水泥和工业副产品硬化弱地面的固溶组成及其制造方法

摘要

PURPOSE: A solidifying composition for soft ground using early strength cement and industrial byproduct minerals is provided to be effectively used in soil improvement by using surface soil stabilization method during winter and to use massive industrial byproduct minerals, thereby reducing the cost of materials for solidification agent and keeping up with the current use trend of low-carbon materials. CONSTITUTION: A solidifying composition for soft ground using early strength cement and industrial byproduct minerals comprises 35 to 60 wt% early strength cement, 20 to 30 wt% ground granulated blast-furnace slag, 5 to 10 wt% fly ash, and 15 to 25 wt% desulfurized gypsum which is byproduct from steel production or oil refinery. The early strength cement is made by crushing gypsum mixed with early strength cement clinker which includes 0.65 to 0.85 wt% sulfur trioxide and has a lime saturation factor of 91.5 to 93.5% with respect to the total weight of the solidifying composition. The fineness of the early strength cement is 5,000 to 5,200 cm2/g.
机译:目的:提供一种使用早强水泥和工业副产品矿物的软土固化组合物,可在冬季通过使用表面土壤稳定化方法有效地用于土壤改良,并使用大量工业副产品矿物,从而降低了固化剂材料的成本并紧跟目前低碳材料的使用趋势。组成:使用早强水泥和工业副产品矿物的软土固化组合物,包括35至60 wt%的早强水泥,20至30 wt%的粒状高炉矿渣,5至10 wt%的粉煤灰和15至25 wt%脱硫石膏,是钢铁生产或炼油厂的副产品。早强水泥是通过将石膏与早强水泥熟料混合而制成的,该熟料包含0.65至0.85 wt%的三氧化硫,且相对于固化组合物的总重量而言,其石灰饱和系数为91.5至93.5%。早强水泥的细度为5,000至5,200 cm2 / g。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号