PURPOSE: A low carbon warm-mix modified regeneration asphalt mixture comprises warm-mix modified asphalt and an asphalt recycling additive, thereby lowering a temperature under 30 deg C in a process. CONSTITUTION: A low carbon warm-mix regeneration modified asphalt mixture comprises the following: 2-8 wt% of warm-mix modified aspha and 0.1-3 wt% of a regeneration additive for warm-mix to 100 wt% of an aggregate mixture comprising 25-95 wt% of recycled aggregate, 4-74 wt% of new aggregate, and 1-6 wt% of filler. The warm-mix regeneration modified asphalt mixture is produced and used at 130-140 deg C. The warm-mix modified asphalt comprises the following: 75-95 wt% of straight asphalt having a penetration grade of 60-80; 0.5-5.0 wt% of an amine-based additive; and 4.5-20.0 wt% of a modifier. The modifier comprises the following: sulfur, paraffin wax, microwax, Styrene butadiene styrene (SBS), and tire powder. The regeneration additive for warm-mix comprises the following: 1.0-10 wt% of a vegetable oil-wax mixture; 75-98 wt% of an antioxidant-straight asphalt mixture; and 1-15 wt% of an adhesion promoter. The antioxidant is more than one among phenyl- -naphthylamine, aromatic amines, and hydroquinone.
机译:目的:一种低碳的热混合改性再生沥青混合物,包括热混合改性沥青和沥青回收添加剂,从而在过程中将温度降低到30摄氏度以下。组成:一种低碳的热拌再生改性沥青混合物,包括:2-8 wt%的热拌改性沥青;和用于热混合的再生添加剂的0.1-3重量%至100重量%的骨料混合物,所述骨料混合物包含25-95重量%的再循环骨料,4-74重量%的新骨料和1-6重量%的填料。在130-140℃下生产和使用该热拌再生改性沥青混合物。该热拌改性沥青包含以下物质:75-95 wt%的渗透度为60-80的直馏沥青; 0.5-5.0 wt%的胺基添加剂;和4.5-20.0重量%的改性剂。改性剂包括以下物质:硫,石蜡,微蜡,苯乙烯丁二烯苯乙烯(SBS)和轮胎粉末。用于温拌的再生添加剂包括:1.0-10重量%的植物油-蜡混合物;和75-98 wt%的抗氧化剂-纯沥青混合物;和1-15wt%的增粘剂。抗氧化剂是苯基-萘胺,芳族胺和对苯二酚中的一种以上。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号