FIELD: oil and gas industry.;SUBSTANCE: in preparation method of grouting mortar for insulation and prevention of earthfalls in cavernous part of the shaft of wells, and mainly gently sloping and horizontal ones, by mixing Portland cement, clay powder, water and additives, which differs by the fact that as additives there used are silicates of alkali metals and derivatives of higher fatty acids, which are obtained at processing of wood or oil resins and tar oils. First, water solution of silicates of alkali metals is prepared by introducing the latter to water. Then, derivatives of higher fatty acids, which are obtained at processing of wood or oil resins and tar oils, are introduced to the above water solution. Mixture is mixed during at least 40 minutes. Then, while stirring, clay powder is added and mixed during 10-20 minutes, and then Portland cement is added, and the mixture is stirred during not less than 30 minutes. Clay powder providing the yield of clay mud with viscosity of 20 mPa*s of not less than 16 m3/t is used as clay powder at the following component ratio, wt %: silicates of alkali metals 10-20, Portland cement 20-70, the above derivatives of higher fatty acids 2-5, the above clay powder 10-25, and water 100.;EFFECT: excluding sedimentation phenomena, diffusion and sagging of an insulating or fixing bridge, including at construction of wells with big deviation of the well shaft from vertical plane; providing complete filling of an inclined shaft of the well, possibility of forming the structure and hardening of the mortar immediately in the zone of earthfalls; providing hydrophobisation and inhibition of the formation rocks.;2 cl, 3 tbl, 3 dwg
机译:领域:石油和天然气工业;物质:通过混合波特兰水泥,粘土粉,水和添加剂,在井筒的海绵状部位(主要是缓坡和水平井)中进行绝缘和防止塌陷的灌浆砂浆的制备方法的不同之处在于,所使用的添加剂是碱金属的硅酸盐和高级脂肪酸的衍生物,它们是在木材或油性树脂和焦油的加工过程中获得的。首先,通过将碱金属硅酸盐引入水中来制备碱金属硅酸盐的水溶液。然后,将在木材或油性树脂和焦油的加工中获得的高级脂肪酸的衍生物引入上述水溶液中。将混合物混合至少40分钟。然后,在搅拌的同时,添加粘土粉并在10-20分钟内混合,然后添加波特兰水泥,并且将混合物搅拌不少于30分钟。黏土粉的黏度为20 mPa * s不小于16 m 3 / t,其黏土粉的重量百分比如下:碱金属硅酸盐10 -20,波特兰水泥20-70,上述高级脂肪酸2-5的衍生物,上述粘土粉10-25和水100。效果:不包括沉降现象,绝缘或固定桥的扩散和流挂,包括在井筒与垂直平面有较大偏差的井中施工;提供井斜井的完全填充,有可能在塌方区​​域立即形成结构并硬化砂浆;提供疏水作用并抑制地层岩石。; 2 cl,3 tbl,3 dwg

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号