PPROBLEM TO BE SOLVED: To provide a curing agent for a two-pack type polyurethane resin coating material, which is excellent in solubility to low-polarity organic solvents and with which a coating film having excellent solvent resistance and tensile breaking elongation is obtained, to provide a method for producing the same, and to provide a two-pack type polyurethane resin coating material. PSOLUTION: The curing agent contains, as a main component, a modified polyisocyanate obtained by modifying a polyisocyanate with a modification agent having a hydroxy group and a functional group having catalytic activity in the reaction with a main agent having an active hydrogen and a polyether polyol. The modification agent is a hydroxy group-containing amine compound or a hydroxy group-containing acid compound. The polyisocyanate is obtained by reacting an isocyanate and a 3-20C monoalcohol, and preferably contains at least an allophanate group, and more preferably has a molar ratio of allophanate group to isocyanurate group of 100/0 to 30/70. PCOPYRIGHT: (C)2011,JPO&INPIT
机译:

要解决的问题:提供用于两包装型聚氨酯树脂涂料的固化剂,该固化剂对低极性有机溶剂的溶解性优异,并且具有优异的耐溶剂性和拉伸断裂伸长率的涂膜所获得的聚合物,提供其制备方法,并提供两包装型聚氨酯树脂涂料。

解决方案:固化剂包含作为主要成分的改性多异氰酸酯,该改性多异氰酸酯是通过在与具有活泼氢的主剂反应中用具有羟基和催化活性的改性剂对多异氰酸酯进行改性而获得的。聚醚多元醇。改性剂是含羟基的胺化合物或含羟基的酸化合物。多异氰酸酯是通过使异氰酸酯与3〜20℃的一元醇反应而得到的,优选至少含有脲基甲酸酯基,更优选脲基甲酸酯基与异氰脲酸酯基的摩尔比为100/0〜30/70。