PROBLEM TO BE SOLVED: To provide a soft-magnetic steel material excellent in wear resistance and magnetic properties after being nitrided.;SOLUTION: The soft-magnetic steel material for nitration contains C:0.001 to 0.020% (% means mass%. The same hereafter.), Si:0.1% or less (not including 0%), Mn:0.1 to 0.5%, P:0.02% or less (not including 0%), S:0.02% or less (not including 0%), Cu:0.1% or less (not including 0%), Ni:0.1% or less (not including 0%), Al:0.040% or less (not including 0%), N:0.0040% or less (not including 0%), further Nb:0.015 to 0.08% and/or Ti:0.01 to 0.1% so as to satisfy expression (1), and the balance iron with inevitable impurities, and the steel structure of the soft-magnetic steel material for nitration is a ferrite single phase structure. 8≤([Nb]+2×[Ti])/[N]≤60...(1), where [Nb], [Ti] and [N] are represents a content (mass%) of Nb, Ti and N, respectively.;COPYRIGHT: (C)2014,JPO&INPIT
机译:要解决的问题:提供一种氮化后的耐磨性和磁性能优良的软磁钢材料;解决方案:用于硝化的软磁钢材料的C:0.001至0.020%(%表示质量%。相同Si:0.1%以下(不包含0%),Mn:0.1〜0.5%,P:0.02%以下(不包含0%),S:0.02%以下(不包含0%), Cu:0.1%以下(不包含0%),Ni:0.1%以下(不包含0%),Al:0.040%以下(不包含0%),N:0.0040%以下(不包含0%) ),为了满足式(1),进一步使Nb:0.015〜0.08%和/或Ti:0.01〜0.1%,余量的铁具有不可避免的杂质,硝化用软磁性钢材的钢组织为α。铁氧体单相结构。 8≤([Nb] + 2×[Ti])/ [N]≤60...(1),其中[Nb],[Ti]和[N]表示Nb,Ti的含量(质量%)和N,分别。;版权:(C)2014,JPO&INPIT

著录项

  • 公开/公告号JP2014074234A

    专利类型

  • 公开/公告日2014-04-24

    原文格式PDF

  • 申请/专利权人 KOBE STEEL LTD;

    申请/专利号JP20130260342

  • 申请日2013-12-17

  • 分类号C22C38/00;C22C38/16;C21D1/06;C23C8/32;H01F1/14;C21D8/12;

  • 国家 JP

  • 入库时间 2022-08-21 16:16:34

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号