首页> 外国专利> CUBIC BORON NITRIDE COMPOSITE POLYCRYSTAL, PRODUCTION METHOD THEREOF, AND CUTTING TOOL, ABRASION RESISTANCE TOOL AND GRINDING TOOL EACH EQUIPPED WITH THE CUBIC BORON NITRIDE COMPOSITE POLYCRYSTAL

CUBIC BORON NITRIDE COMPOSITE POLYCRYSTAL, PRODUCTION METHOD THEREOF, AND CUTTING TOOL, ABRASION RESISTANCE TOOL AND GRINDING TOOL EACH EQUIPPED WITH THE CUBIC BORON NITRIDE COMPOSITE POLYCRYSTAL

机译:立方氮化硼复合聚碳酸酯,其制备方法以及切割工具,耐磨性工具和磨削工具

摘要

PROBLEM TO BE SOLVED: To provide a cubic boron nitride composite polycrystal having excellent abrasion resistance, a production method thereof, and a cutting tool, an abrasion resistant tool and a grinding tool each equipped with the polycrystal.;SOLUTION: A cubic boron nitride composite polycrystal 10 comprises: granular cubic boron nitride 1; and laminar boron nitride 3. The laminar boron nitride 3 has contact with the granular cubic boron nitride 1, and tabular boron nitride 2 is laminated on the laminar boron nitride 3. The tabular boron nitride 2 at least includes one of cubic boron nitride and wurtzite type boron nitride. The area of the tabular boron nitride 2 is 0.5% or more and 30% or less, in an area ratio to the whole surface area.;COPYRIGHT: (C)2014,JPO&INPIT
机译:解决的问题:提供一种具有优异的耐磨性的立方氮化硼复合物多晶,其制造方法以及均配备有该多晶的切割工具,耐磨工具和研磨工具。多晶10包括:粒状立方氮化硼1;和层状氮化硼3与粒状立方氮化硼1接触,并且在层状氮化硼3上层叠有板状氮化硼2。板状氮化硼2至少包括立方氮化硼和纤锌矿中的一种。型氮化硼。板状氮化硼2的面积相对于整个表面积的面积比为0.5%以上且30%以下。; COPYRIGHT:(C)2014,JPO&INPIT

著录项

  • 公开/公告号JP2014080323A

    专利类型

  • 公开/公告日2014-05-08

    原文格式PDF

  • 申请/专利权人 SUMITOMO ELECTRIC IND LTD;

    申请/专利号JP20120228816

  • 发明设计人 ISHIDA TAKESHI;SUMIYA HITOSHI;

    申请日2012-10-16

  • 分类号C04B35/583;B23B27/14;B24D3/00;C01B21/064;

  • 国家 JP

  • 入库时间 2022-08-21 16:15:23