PROBLEM TO BE SOLVED: To provide a resin composition superior in fluidity and post-processability, easy in molding an injection produce of a large one and a thin film, and superior in rigidity and impact strength by an excellent characteristic of high crystalline polypropylene and an ethylene-propylene copolymer.;SOLUTION: This ethylene-propylene block copolymer-based polypropylene resin composition having a melt index of 80-120 g/10 min, includes (A) 80-95 mass% of high crystalline homo-polypropylene having an isotactic pentad fraction of 96% or more and (B) 5 to 20 mass% of an ethylene-propylene elastic copolymer having the mole ratio of ethylene/(ethylene + propylene) of 0.15-0.40, and includes 100 mass part of a polypropylene resin being 0.09-0.33 in the ratio (A/B) of absolute viscosity of high crystalline homo-polypropylene (A) to the ethylene-propylene elastic copolymer (B) and (C) 0.05-0.3 mass part of a nucleating agent.;COPYRIGHT: (C)2009,JPO&INPIT
机译:要解决的问题:提供一种树脂组合物,其流动性和后加工性优异,易于模塑大片和薄膜的注射制品,并具有高结晶聚丙烯和高分子量聚丙烯的优良特性,具有优异的刚性和冲击强度。乙烯-丙烯共聚物;解决方案:该基于乙烯-丙烯嵌段共聚物的聚丙烯树脂组合物具有80-120 g / 10 min的熔融指数,包含(A)80-95质量%的具有全同立构规整度的高结晶均聚丙烯乙烯/(乙烯+丙烯)的摩尔比为0.15〜0.40的乙烯-丙烯弹性共聚物的96%以上,(B)5〜20质量%的五单元组分,其中,聚丙烯树脂100质量份为高结晶均聚丙烯(A)与乙烯-丙烯弹性共聚物(B)的绝对粘度之比(A / B)和(C)0.05-0.3质量份成核剂,其比值(A / B)为0.09-0.33。 (C)2009,日本特许厅&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号