首页> 外国专利> Production manner, and the spinel of spinel precursive body sol add to the aqueous solution of the temperature 80 - the 95 which include

Production manner, and the spinel of spinel precursive body sol add to the aqueous solution of the temperature 80 - the 95 which include

机译:生产方式,将尖晶石前体溶胶的尖晶石添加到温度为80〜95℃的水溶液中,包括

摘要

PROBLEM TO BE SOLVED: To provide a stable sol capable of forming a coating film that is hardly reduced by aluminum and does not undergo phase change, even when heated to an elevated temperature, and a method for manufacturing the sol.;SOLUTION: The spinel precursor sol comprises colloid particles of a reaction product of an aluminum alkoxide hydrolysate and magnesium ion that are dispersed in an aqueous solvent with a pH of 1-5 and forms a spinel at 300-400°C. The method for manufacturing the same comprises; adding an aluminum alkoxide to an aqueous solution of a magnesium salt, without dissolving the aluminum alkoxide in an organic solvent, and hydrolyzing the same at 80-95°C; and deflocculating the resulting reaction product of the aluminum alkoxide hydrolysate and a magnesium ion by adjusting the pH of the aqueous solvent to 1-5.;COPYRIGHT: (C)2010,JPO&INPIT
机译:解决的问题:提供一种稳定的溶胶,该溶胶能够形成几乎不会被铝还原并且即使加热到高温也不会发生相变的涂膜,以及制备该溶胶的方法。前体溶胶包含醇铝水解产物和镁离子的反应产物的胶体颗粒,其分散在pH为1-5的水性溶剂中并在300-400℃下形成尖晶石。所述制造方法包括:在不将烷氧基铝溶解在有机溶剂中的情况下,将烷氧基铝添加到镁盐的水溶液中,并在80-95℃下水解。通过将水相溶剂的pH值调节至1-5,使醇铝水解产物与镁离子的反应产物脱絮凝;版权所有:(C)2010,JPO&INPIT

著录项

  • 公开/公告号JP5554934B2

    专利类型

  • 公开/公告日2014-07-23

    原文格式PDF

  • 申请/专利权人

    申请/专利号JP20090062155

  • 发明设计人

    申请日2009-03-15

  • 分类号C01F7/16;C01G23/00;

  • 国家 JP

  • 入库时间 2022-08-21 16:15:05