首页> 外国专利> Hot stretch straightening of high strength age hardened metallic form and straightened age hardened metallic form

Hot stretch straightening of high strength age hardened metallic form and straightened age hardened metallic form

机译:高强度时效硬化金属模和时效硬化金属模的热拉伸矫直

摘要

A method for straightening an age hardened metallic form includes heating an age hardened metallic form comprising one of a titanium alloy, a nickel alloy, an aluminum alloy, and a ferrous alloy to a straightening temperature of at least 25° F. below the age hardening temperature, and applying an elongation tensile stress for a time sufficient to elongate and straighten the form. The elongation tensile stress is at least 20% of the yield stress and not equal to or greater than the yield stress at the straightening temperature. The straightened form deviates from straight by no greater than 0.125 inch over any 5 foot length or shorter length. The straightened form is cooled while simultaneously applying a cooling tensile stress that balances the thermal cooling stress in the metallic form to thereby maintain a deviation from straight of no greater than 0.125 inch over any 5 foot length or shorter length.
机译:用于矫正时效硬化的金属模板的方法包括将包括钛合金,镍合金,铝合金和铁合金中的一种的时效硬化的金属模板加热到比时效硬化至少25°F的矫直温度。温度,并施加足以使模板拉直和拉直的时间的拉伸拉应力。伸长拉伸应力为屈服应力的至少20%,并且在矫直温度下不等于或大于屈服应力。在任何5英尺或更短的长度内,拉直的形状与直线的偏差不大于0.125英寸。矫直的模板被冷却,同时施加冷却拉伸应力以平衡金属形式的热冷却应力,从而在任何5英尺或更短的长度上保持与直线的偏差不大于0.125英寸。

著录项

  • 公开/公告号US8834653B2

    专利类型

  • 公开/公告日2014-09-16

    原文格式PDF

  • 申请/专利权人 ATI PROPERTIES INC.;

    申请/专利号US201313933222

  • 发明设计人 DAVID J. BRYAN;

    申请日2013-07-02

  • 分类号C21D8;C22F1/18;B21D3/12;

  • 国家 US

  • 入库时间 2022-08-21 16:05:40