首页> 外国专利> LOW YIELD RATIO HIGH-STRENGTH HOT-DIP GALVANIZED STEEL SHEET, LOW YIELD RATIO HIGH-STRENGTH HOT-DIP GALVANNEALED STEEL SHEET, METHOD FOR MANUFACTURING LOW YIELD RATIO HIGH-STRENGTH HOT-DIP GALVANIZED STEEL SHEET, AND METHOD FOR MANUFACTURING LOW YIELD RATIO HIGH-STRENGTH HOT-DIP GALVANNEALED STEEL SHEET

LOW YIELD RATIO HIGH-STRENGTH HOT-DIP GALVANIZED STEEL SHEET, LOW YIELD RATIO HIGH-STRENGTH HOT-DIP GALVANNEALED STEEL SHEET, METHOD FOR MANUFACTURING LOW YIELD RATIO HIGH-STRENGTH HOT-DIP GALVANIZED STEEL SHEET, AND METHOD FOR MANUFACTURING LOW YIELD RATIO HIGH-STRENGTH HOT-DIP GALVANNEALED STEEL SHEET

机译:低屈服比高强度热浸镀锌钢板,低屈服比高强度热浸镀锌钢板,制造低屈服比高强度热浸镀锌钢板的方法,低密度比高强度热浸镀锌钢板,低屈服比高强度热浸镀锌钢板,低屈服比高强度热浸镀锌钢板,制造方法强度热浸镀锌钢板

摘要

A low yield ratio high-strength hot-dip galvanized steel sheet includes as chemical composition, by % by mass, 0.03% to 0.20% C, 1.0% or less Si, more than 1.5% to 3.0% Mn, 0.10% or less P, 0.05% or less S, 0.10% or less Al, 0.010% or less N, 0.5% or less Cr, and 0.01% to 0.50% Mo, and the balance Fe with inevitable impurities, and also includes a structure including a ferrite and a second phase. The ferrite has an area ratio of 50% or more, and the second phase includes martensite whose area ratio is in the range from 7% to less than 25%. The thickness of a band-like structure formed by the second phase satisfies the predetermined equation.
机译:低屈服比高强度热浸镀锌钢板以质量%计包含0.03〜0.20%的C,1.0%以下的Si,大于1.5%〜3.0%的Mn,0.10%以下的P作为化学组成。 S,0.05%以下的S,0.10%以下的Al,0.010%以下的N,0.5%以下的Cr以及0.01%至0.50%的Mo以及余量的Fe具有不可避免的杂质,并且还具有包括铁素体和第二阶段。铁素体具有50%以上的面积比,并且第二相包括马氏体,其面积比在7%至小于25%的范围内。由第二相形成的带状结构的厚度满足预定公式。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号