the invention concerns the manufacture of granules of waste dust perlitowego, intended for use in construction, among others. in tynkarskich thin-film devices. a way is that to granulatora lining is dust perlitowy about uziarnieniu below 0.5 mm and natryskuje binder, in the form of an aqueous dispersion of the polymer.apply 50 - 150 parts by weight per 100 parts by weight of the binder. in the initial stage of the process of apply turnover drum 1 - 20 rpm, and subsequently, during 3 - 15 minutes, increasing to 50 - 100 rpm, and at the same time, heats the radiacyjnie mass in the entire volume of the radiation infrared, to the temperature not higher than 80u00b0c.the mixing is continued for 5 to 30 minutes, after which the drought konwekcyjnie stream air for a period of 60 to 180 minutes, keeping the temperature of forced air at 40 - 80u00b0c until spherical granules of 0.5 - 1.5 mm, and the moisture content below 1.5% by weight, of what jmniej 70% by weight of dust perlitowego.
机译:本发明涉及用于建筑的废粉尘颗粒的制造,该颗粒旨在用于建筑等。在tynkarskich薄膜设备中。一种方式是,造粒机衬里是粉尘状的粉尘,约小于0.5mm的uziarnieniu和natryskuje粘合剂,以聚合物的水分散体形式。每100重量份的粘合剂施加50-150重量份。在应用周转鼓的过程的初始阶段,转速为1-20 rpm,随后在3-15分钟内,增加到50-100 rpm,并同时加热整个辐射红外线中的radiacyjnie质量,直到温度不高于80 u00b0c。继续混合5至30分钟,然后干旱的konwekcyjnie气流持续60至180分钟,将强制空气的温度保持在40-80 u00b0c,直到球形颗粒为0.5-1.5毫米,且水分含量低于1.5重量%,是粉尘的70%重量。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号