A method for extracting vanadium from shale, the method including: a) grinding the shale into fine powders, mixing the fine powders with an additive in a mass ratio of 1:0.04-0.12 to yield a mixture, heating the mixture to a temperature of between 850 and 950° C. at a heating rate of 5-9° C./min, and baking the mixture for between 30 and 90 min; b) immersing the product in water and acid respectively to yield a first solution and a second solution, combining the two solutions, and performing ion exchange adsorption on the combined solution using a styrene-divinylbenzene based macroporous anion-exchange resin; and c) performing desorption, purification, and precipitation to yield poly ammonium vanadate, and calcining the poly ammonium vanadate at a temperature of between 450 and 530° C. for between 20 and 50 min to yield V2O5.
机译:一种从页岩中提取钒的方法,该方法包括:a)将页岩磨成细粉,将细粉与添加剂以质量比1:0.04-0.12混合以产生混合物,将混合物加热至在850至950℃之间,以5-9℃/ min的加热速率,将混合物烘烤30至90min; b)将产物分别浸入水和酸中,得到第一溶液和第二溶液,将两种溶液合并,并使用苯乙烯-二乙烯基苯基大孔阴离子交换树脂对合并的溶液进行离子交换吸附; c)进行解吸,纯化和沉淀,得到聚钒酸铵,并在450-530℃的温度下煅烧聚钒酸铵20-50分钟,得到V2O5。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号