A geopolymer concrete formed by mixing about 3% to about 43% by weight incinerator fly ash, about 3% to about 35% by weight coal fly ash, about 7% to about 38% by weight alkaline activator liquid, and about 31 % to about 70% by weight aggregate. The incinerator fly ash may be derived from a solid waste incinerator facility. The alkaline activator liquid may include a sodium hydroxide solution and sodium silicate. The aggregate may include a fine aggregate, such as sand, and a coarse aggregate, such as gravel.
机译:通过混合按重量计约3%至约43%的焚烧粉煤灰,按重量计约3%至约35%的煤粉煤灰,按重量计约7%至约38%的碱性活化剂液体和按重量计约31%的土工聚合物混凝土约占总重量的70%。焚化炉的飞灰可以来自固体废物焚化炉设施。碱性活化剂液体可包括氢氧化钠溶液和硅酸钠。骨料可包括细骨料,例如沙子,和粗骨料,例如砾石。