Related are a copper indium sulfide nanoparticles and a preparation method thereof. Copper salts, indium salts and alkane thiol are added to a non-polar organic solvent, and then are heated with stirring under inert gas atmosphere to dissolve until a dark red colloidal solution is obtained. The obtained colloidal solution is cooled to room temperature, and then a polar solvent is added. The copper indium sulfide semiconductor nanoparticles are obtained through centrifugal settling. The obtained copper indium sulfide semiconductor nanoparticles could be further washed and vacuum dried to give copper indium sulfide semiconductor nanoparticle powders. The obtained copper indium sulfide semiconductor nanoparticles have an average particle size of 2 to 10 nm and an emission spectrum of 600 to 800 nm in the near infrared region, quantum efficiency being close to 10%. The yield of the present method is up to 90%.
机译:相关的是铜铟硫纳米颗粒及其制备方法。将铜盐,铟盐和链烷硫醇添加到非极性有机溶剂中,然后在惰性气体气氛下在搅拌下加热以溶解直至获得深红色胶体溶液。将获得的胶体溶液冷却至室温,然后添加极性溶剂。通过离心沉降获得铜铟硫半导体纳米颗粒。可以进一步洗涤获得的铜铟硫半导体纳米颗粒,并真空干燥,得到铜铟硫半导体纳米颗粒粉末。所获得的铜铟硫化物半导体纳米颗粒的平均粒径为2至10nm,并且在近红外区域中的发射光谱为600至800nm,量子效率接近10%。本方法的产率高达90%。

著录项

  • 公开/公告号EP2263977A4

    专利类型

  • 公开/公告日2014-01-29

    原文格式PDF

  • 申请/专利权人 BAYER INTELLECTUAL PROPERTY GMBH;

    申请/专利号EP20090718518

  • 发明设计人 ZHONG HAIZHENG;LI YONGFANG;

    申请日2009-03-06

  • 分类号C01G1/12;C01G3/12;C01G15/00;

  • 国家 EP

  • 入库时间 2022-08-21 15:50:33

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号