首页> 外国专利> White, biaxially oriented polyester film, matt on at least one side and weatherproof, method for its manufacture, and its use

White, biaxially oriented polyester film, matt on at least one side and weatherproof, method for its manufacture, and its use

机译:白色双轴取向聚酯薄膜,至少一侧无光泽且防风雨,其制造方法及其用途

摘要

White, biaxially oriented polyester film comprises at least one white mat base layer containing a white pigment, and at least one white mat top layer containing a white pigment, where the top layer and the base layer in addition to the white pigment comprise particles different from the white pigment having an increased degree of mattness. The particles have an average particle diameter of 2-10 mu m. The top layer and the base layer are present at 1-7 wt.%. The particle diameter and the concentration of the top layer and the base layer are the same or different. White, biaxially oriented polyester film comprises at least one white mat base layer containing a white pigment, and at least one white mat top layer containing a white pigment, where the top layer and the base layer in addition to the white pigment comprise particles different from the white pigment having an increased degree of mattness. The particles have an average particle diameter of 2-10 mu m. The top layer and the base layer are present at 1-7 wt.%. The particle diameter and the concentration of the top layer and the base layer are the same or different. The white pigment in the top layer is present at 2-15 wt.%. The top layer contains a UV-stabilizer in a concentration of 0.3-8 wt.%. An independent claim is included for producing the polyester film, comprising coextruding the individual layers of the film corresponding to melt by a flat die and to form a melt film, where the resultant film is drawn off for solidification on one or more rollers, the film is then biaxially stretched, optionally coated prior to or during stretching, the biaxially stretched film is thermofixed, and optionally surface layer intended for the treatment is corona-or flame-treated and is then rolled up.
机译:白色双轴取向聚酯薄膜包括至少一个包含白色颜料的白色垫基层和至少一个包含白色颜料的白色垫基层,其中除白色颜料外,顶层和基层还包含与具有增加的哑光度的白色颜料。颗粒的平均粒径为2-10μm。顶层和基础层的含量为1-7重量%。顶层和基础层的粒径和浓度相同或不同。白色双轴取向聚酯薄膜包括至少一个包含白色颜料的白色垫基层和至少一个包含白色颜料的白色垫基层,其中除白色颜料外,顶层和基层还包含与具有增加的哑光度的白色颜料。颗粒的平均粒径为2-10μm。顶层和基础层的含量为1-7重量%。顶层和基础层的粒径和浓度相同或不同。顶层中的白色颜料以2-15重量%存在。顶层包含浓度为0.3-8重量%的紫外线稳定剂。包括用于生产聚酯膜的独立权利要求,其包括通过平模共挤出对应于熔体的膜的各个层并形成熔体膜,其中将所得膜拉出以在一个或多个辊上固化,该膜然后将其双轴拉伸,任选在拉伸之前或期间涂布,将双轴拉伸的膜热固,并任选将用于处理的表面层进行电晕或火焰处理,然后卷起。

著录项