Provided is a method for preparing high-purity aluminum by directional solidification, comprising the steps of: providing 4N to 5N aluminum as raw material, heating the same to a temperature of 670 °C to 730 °C, maintaining the temperature for 7 minutes to 80 minutes, cooling the bottom of chamber (3) to allow the aluminum liquid crystallizing in a direction from the bottom to top of the chamber (3) for 1 hour to 8 hours to obtain a crystalline ingot, during the crystallization process of a finished product of crystalline ingot, stirring and heating the aluminum liquid, maintaining a particular temperature gradient of the aluminum liquid, and removing a portion of the crystalline ingot from one end of the ingot, the remaining portion being the high-purity aluminum. Also provided is a smelting furnace, comprising a shell (1), a heating device (2), a chamber (3), a temperature measurement device, a stirring device and a cooling device (6).
机译:提供了一种通过定向凝固制备高纯铝的方法,其包括以下步骤:提供4N至5N铝为原料,将其加热至670°C至730°C的温度,保持该温度7分钟以内。 80分钟,在完成的结晶过程中,冷却腔室(3)的底部以使铝液在从腔室(3)的底部到顶部的方向上结晶1小时至8小时以获得结晶锭。结晶锭的产物,搅拌并加热铝液,保持铝液的特定温度梯度,并从锭的一端除去一部分结晶锭,其余部分是高纯度铝。还提供了一种熔炉,其包括壳体(1),加热装置(2),腔室(3),温度测量装置,搅拌装置和冷却装置(6)。

著录项

  • 公开/公告号EP2743359A1

    专利类型

  • 公开/公告日2014-06-18

    原文格式PDF

  • 申请/专利权人 XINJIANG JOINWORLD CO. LTD.;

    申请/专利号EP20110870784

  • 发明设计人 HONG TAO;NURGUL IMIN;

    申请日2011-12-14

  • 分类号C22B21/06;C22B9/02;

  • 国家 EP

  • 入库时间 2022-08-21 15:45:36

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号