A radical-curable resin composition comprising a urethane methacrylate resin (A), a polyester methacrylate resin (B), and an ethylenically unsaturated monomer having a (meth)acryloyl group (C), characterized in that the urethane methacrylate resin (A) is obtained by reacting a polyisocyanate (a) with a polyether polyol (b) and then reacting the resulting product with a hydroxyalkyl methacrylate, the polyester methacrylate resin (B) is obtained by using 40 mol% or more of adipic acid as an acid component and has a number average molecular weight of 2000 to 4000, and a dicyclopentadiene unsaturated polyester resin (D) as a compatibilizer is contained in an amount of 5 to 25 parts by mass with respect to 100 parts by mass of the total amount of the resin (A) and the resin (B).
机译:一种自由基固化性树脂组合物,其包含氨基甲酸酯甲基丙烯酸酯树脂(A),聚酯甲基丙烯酸酯树脂(B)和具有(甲基)丙烯酰基的烯键式不饱和单体(C),其特征在于,所述氨基甲酸酯甲基丙烯酸酯树脂(A)为通过使多异氰酸酯(a)与聚醚多元醇(b)反应,然后将所得产物与甲基丙烯酸羟烷基酯反应而获得,通过使用40mol%以上的己二酸作为酸成分,得到聚酯甲基丙烯酸酯树脂(B)。相对于100质量份的树脂总量,其数均分子量为2000〜4000,并且作为增容剂的二环戊二烯不饱和聚酯树脂(D)的含量为5〜25质量份。 A)和树脂(B)。

著录项

  • 公开/公告号KR20130132692A

    专利类型

  • 公开/公告日2013-12-05

    原文格式PDF

  • 申请/专利权人 DIC CORPORATION;

    申请/专利号KR20127024206

  • 申请日2011-10-31

  • 分类号C08F290/06;C08L75/16;C08L67/06;C09D4/02;C09D167/06;C09D175/16;

  • 国家 KR

  • 入库时间 2022-08-21 15:44:52

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号