The present invention relates to a method of producing a wholly aromatic polyester production method of the polyamide polymer and the aramid fibers using the same having a variation in the inherent viscosity ever yet extremely high specific viscosity, the wholly aromatic polyamide polymer prepared by the method of the present invention, the polymerization solvent comprising dissolved to prepare a mixed solution of an aromatic diamine; Preparing the prepolymer by the addition of an aromatic halide diethoxy seed to the mixed solution; And further comprising the step of producing the final polymer by further adding the aromatic halide to the seed diethoxy prepolymer, the prepolymer is characterized in that it is a 1.20 to 2.00 molar ratio of aromatic diamine to an aromatic halide diethoxy seed. ; Polyamide, aramid, prepolymer, NMR, the average mole ratio, intrinsic viscosity
机译:本发明涉及一种生产全芳族聚酯的方法,该生产方法是使用聚酰胺树脂和芳族聚酰胺纤维,它们具有比浓对数粘度变化而比粘度非常高的聚酰胺聚合物和芳族聚酰胺纤维,在本发明中,聚合溶剂包括溶解以制备芳族二胺的混合溶液;通过向混合溶液中加入芳族卤代二乙氧基种子制备预聚物;并且进一步包括通过将芳族卤化物进一步添加到种子二乙氧基预聚物中来制备最终聚合物的步骤,该预聚物的特征在于它是芳族二胺与芳族卤化物二乙氧基种子的1.20至2.00摩尔比。 ;聚酰胺,芳纶,预聚物,NMR,平均摩尔比,特性粘度

著录项

  • 公开/公告号KR101337053B1

    专利类型

  • 公开/公告日2013-12-05

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20080050375

  • 发明设计人 한인식;

    申请日2008-05-29

  • 分类号C08G69/28;C08G69/26;C08G69/48;D01F6/60;

  • 国家 KR

  • 入库时间 2022-08-21 15:44:06