PURPOSE: A polyethylene terephthalate fully drawn yarn manufacturing method, a fully drawn yarn, a tire cord manufacturing method and a tire cord using superhigh speed spinning technology are provided to manufacture undrawn yarn by using superhigh speed spinning technology and to minimize a tensile strength loss of the fully drawn yarn. CONSTITUTION: The polyethylene terephthalate fully drawn yarn manufacturing method is as follows. The undrawn yarn is manufactured by melt spinning the polyethylene terephthalate at a speed of 3500 - 5000 m / min, and is drawn at a draw ratio of 1.3 - 2.0 times. A ply yarn is manufactured by using the fully drawn yarn. The ply yarn is dipped in an adhesive solution and is heat-treated.
机译:目的:提供一种使用超高速纺丝技术的聚对苯二甲酸乙二醇酯全拉伸丝的制造方法,一种全拉伸丝,一种轮胎帘线的制造方法和一种轮胎帘线,以通过使用超高速纺丝技术来制造未拉伸丝,并最大程度地降低拉伸强度损失。完全拉伸的纱线。组成:聚对苯二甲酸乙二酯全拉伸丝的制造方法如下。未拉伸丝是通过将聚对苯二甲酸乙二醇酯以3500-5000m / min的速度熔融纺丝而制造的,并且以1.3-2.0倍的拉伸比进行拉伸。通过使用完全拉伸的纱线来制造股线。将帘线纱线浸入粘合剂溶液中并进行热处理。

著录项

  • 公开/公告号KR101338505B1

    专利类型

  • 公开/公告日2013-12-10

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20090135667

  • 发明设计人 박성호;정일;김기웅;

    申请日2009-12-31

  • 分类号D01F6/62;D02G3/48;B60C9/12;

  • 国家 KR

  • 入库时间 2022-08-21 15:44:07

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号