In the present invention, for removing and having treated the compound, at low cost, high-efficient of stubborn organic pollutant, nanosize metal oxide synthetic soapstone compound is provided to treat stubborn organic pollutant compound and its manufacturing method, can be applied to high-efficient purification contaminated soil and underground water and the water that above-mentioned removing endocrine has a brick in one's hat. Complex composition by zinc oxide, hectorite, lithium metasilicate, in polyvinyl alcohol water solution, calcium carbonate and specific ratios. The manufacturing method includes the steps that forming mixture, by the zinc oxide of 25-65 weight %, the synthetic soapstone aqueous solution of 19-45 weight %, and the 2. of 5-10 weight %0 M lithium silicate aqueous solutions in the polyvinyl alcohol water solution of 5-10 weight ratios and the calcium carbonate of 6-10 weight % and are in slurry; In molding step, the paste mixture is at graininess; With the blends of dried granules. ;The 2014 of copyright KIPO submissions
机译:在本发明中,为了去除和处理该化合物,以低成本,高效率的顽固有机污染物,提供了纳米级金属氧化物合成皂石化合物来处理顽固有机污染物及其制备方法,可应用于高高效净化受污染的土壤和地下水,以及上述去除内分泌的水都戴上帽子。由氧化锌,锂蒙脱石,偏硅酸锂,聚乙烯醇水溶液,碳酸钙和特定比例组成的复合物。该制造方法包括以下步骤:将25-65重量%的氧化锌,19-45重量%的合成皂石水溶液和5-10重量%的2.0M硅酸锂水溶液形成混合物。浆液为5-10重量比的聚乙烯醇水溶液和6-10重量%的碳酸钙。在成型步骤中,糊状混合物呈颗粒状;与干颗粒的混合物。 ; 2014年版权KIPO提交文件

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号