The present invention relates to a complex copper ore beneficiation method using leaching and a precipitate. According to the present invention, the complex copper ore beneficiation method for manufacturing a copper concentrate from a copper complex ore including copper containing a mineral, and a gangue mineral including talcum comprises: a talcum removing step for removing talcum since talcum and copper containing a mineral are separated by sinking the copper containing a mineral into an inside of pulp and floating the talcum through ore dressing by floatation about a copper complex ore passing through a crushing step and a smashing step; a copper leaching step for leaching copper inside copper containing a mineral by inserting an acid inside pulp including a copper complex ore where talcum is removed; a copper precipitate step for forming copper sulfide by injecting a sulfide precipitant into the pulp where copper is leached; and a copper ore manufacturing step for separating copper sulfide by floating copper sulfide with hydro phobic properties through a floatation about pulp, and sinking other gangue minerals into an inside of pulp. [Reference numerals] (AA) Copper complex ore; (BB) Crushing and smashing; (C1) Talcum removing; (C2) Foaming agent : oil; (C3) Foaming agent : MIBC; (DD) Float product : talcum; (EE) Sink product; (F1) Copper leaching step; (F2) Leaching agent : an inorganic acid (H_2SO_4, HNO_3, and HCI etc.); (F3) Amount used : 2-3 equivalent comparing with contents of a copper ore; (G1) Copper precipitate step; (G2) Precipitant : a sulfide precipitant (Na_2S, CaS, and (NH_4)_2S etc.); (G3) Amount used : 1-3 equivalent comparing with contents of a copper ore; (H1) Manufacture a first concentrate; (H2,K2) Collector; (H3,K3) Xanthate; (H4,K4) Foaming agent; (II) Concentrates 1; (JJ) Tailing; (K1) Manufacture a second concentrate; (LL) Concentrates 2; (MM) Middling
机译:本发明涉及一种使用浸出和沉淀物的复杂铜矿选矿方法。根据本发明,用于由包含矿物质的铜和包含滑石的脉石矿物的铜复合矿制造铜精矿的复合铜矿选矿方法包括:滑石去除步骤,用于去除滑石,因为滑石和含铜的矿物通过将含矿物质的铜下沉到纸浆内部并通过选矿使滑石浮选,该滑石通过在压碎步骤和粉碎步骤中的铜络合物矿石上的浮选而分离。铜浸出步骤,用于通过将酸插入包含去除了滑石的铜配合矿的纸浆中来在包含矿物质的铜中浸出铜;铜沉淀步骤,用于通过将硫化物沉淀物注入浸有铜的纸浆中而形成硫化铜。铜矿的制造步骤,其是通过在纸浆上进行浮选,使具有疏水性的硫化铜浮选而分离硫化铜,并将其他脉石矿物沉入纸浆内部。 [附图标记](AA)铜络合物矿石; (BB)压碎和粉碎; (C1)滑石粉去除; (C2)发泡剂:油; (C3)发泡剂:MIBC; (DD)浮游产品:滑石; (EE)水槽产品; (F1)铜浸出步骤; (F2)浸出剂:无机酸(H_2SO_4,HNO_3和HCl等); (F3)使用量:与铜矿石的含量相比为2-3当量; (G1)铜沉淀步骤; (G2)沉淀剂:硫化物沉淀剂(Na_2S,CaS和(NH_4)_2S等); (G3)使用量:与铜矿石的含量相比为1-3当量; (H1)制造第一浓缩物; (H2,K2)收集器; (H3,K3)黄药(H4,K4)发泡剂; (二)浓缩液1; (JJ)尾矿; (K1)制造第二浓缩物; (LL)浓缩液2; (MM)中级

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号