摘要

PROBLEM TO BE SOLVED: To provide a high strength steel sheet which is excellent in low temperature toughness at the HAZ of a joint portion even while having the tensile strength of 980 MPa or more.SOLUTION: The steel sheet contains 0.12-0.16% (meaning mass%, and the same hereinafter) of C, 0.05-0.5% of Si, 0.8-1.2% of Mn, 0.01-0.07% of Al, 0.5-0.8% of Mo, 0.025-0.08% of Nb, 0.0004-0.002% of B, and 0.8% or less of Cr and/or 0.06% or less of V, respectively, and the balance comprising iron and inevitable impurities. An MP value specified by equation (1) is 0.550 or larger, and a carbon equivalent Ceq specified by equation (2) is 0.63% or less, wherein equation (1) : MP value=(12/[C])×(([Mo]/96)+([Nb]/93)) and equation (2): Ceq=[C]+[Mn]/6+([Cr]+[Mo]+[V])/5+([Cu]+[Ni])/15.
机译:解决的问题:提供即使在抗拉强度为980MPa以上的情况下,接头部的HAZ的低温韧性也优异的高强度钢板。 C,0.05-0.5%Si,0.8-1.2%Mn,0.01-0.07%Al,0.5-0.8%Mo,0.025-0.08%Nb,0.0004-0.002% B分别为0.8%,Cr为0.8%以下,V为0.06%以下,其余为铁和不可避免的杂质。由式(1)指定的MP值为0.550以上,由式(2)指定的碳当量Ceq为0.63%以下,式(1):MP值=(12 / [C])×(( [Mo] / 96)+([Nb] / 93))和公式(2):Ceq = [C] + [Mn] / 6 +([Cr] + [Mo] + [V])/ 5+( [Cu] + [Ni])/ 15。

著录项

  • 公开/公告号KR101365351B1

    专利类型

  • 公开/公告日2014-02-19

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20110098810

  • 发明设计人 가리야자키 마코토;

    申请日2011-09-29

  • 分类号C22C38;C22C38/14;C22C38/54;

  • 国家 KR

  • 入库时间 2022-08-21 15:41:26

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号