The present invention relates to a production method of a high performance carbon fiber using a polyacrylonitrile fiber for fabrics comprising the following steps: an elongation step of elongating the polyacrylonitrile (PAN) fiber for fabrics using more than one process selected from hot water elongation and heat elongation to obtain an elongated polyacrylonitrile (PAN) fiber; oxidizing and stabilizing the elongated polyacrylonitrile (PAN) fiber; and carbonizing the oxidized and stabilized elongated polyacrylonitrile (PAN) fiber. According to the present invention, Using the polyacrylonitrile fiber (PAN) for fabrics, which is not suitable for a precursor of the carbon fiber through hot water elongation and/or heat elongation, the high performance carbon fiber having the proper fiber diameter, high degree of polymer chain orientation, and mechanical strength is obtained. The price of the carbon fiber is capable of decreased by using the polyacrylonitrile fiber (PAN) for fabrics.
机译:本发明涉及使用用于织物的聚丙烯腈纤维的高性能碳纤维的生产方法,其包括以下步骤:延伸步骤,其使用选自热水延伸和加热中的一种以上方法来延伸用于织物的聚丙烯腈(PAN)纤维。伸长以获得伸长的聚丙烯腈(PAN)纤维;氧化和稳定细长聚丙烯腈(PAN)纤维;使碳化并稳定的细长聚丙烯腈(PAN)纤维碳化。根据本发明,使用不适用于通过热水伸长和/或热伸长的碳纤维前体的织物用聚丙烯腈纤维(PAN),可以得到具有适当纤维直径,高程度的高性能碳纤维。聚合物链取向的变化,获得机械强度。通过将聚丙烯腈纤维(PAN)用于织物,能够降低碳纤维的价格。

著录项

  • 公开/公告号KR101395811B1

    专利类型

  • 公开/公告日2014-05-16

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20120054164

  • 申请日2012-05-22

  • 分类号D01F9/22;D01F6/18;D02J1/22;D06M10;

  • 国家 KR

  • 入库时间 2022-08-21 15:40:58

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号